Igwe anaghị agba nchara Electrode AWS A5.4 E2553-16 Stick Electrodes na Titanium-Calcium mkpuchi

Nkọwa dị mkpirikpi:

AF2553-16 (AWS E2553-16) bụ nitrogen nwere duplex igwe anaghị agba nchara electrode nwere titanium-calcium mkpuchi.


Nkọwa ngwaahịa

Mkpado ngwaahịa

Igwe anaghị agba ncharaElectrode

AF2553-16

GB/T E2553-16

AWS A5.4 E2553-16

Nkọwa: AF2553-16 bụ igwe anaghị agba nchara duplex nitrogen nwere mkpuchi titanium-calcium.Enwere ike iji ya maka ma AC na DC na arụmọrụ arụmọrụ dị mma.N'ihi na ọ nwere molybdenum na nitrogen, na carbon ọdịnaya dị oke ala, metal ahụ etinyere nwere ezigbo nguzogide mgbape na nguzogide corrosion, karịsịa nrụgide corrosion nguzogide.

Ngwa: Ọ na-eji maka ịgbado ọkụ duplex igwe anaghị agba nchara na a chromium ọdịnaya nke banyere 25%, dị ka 022Cr25Ni7Mo4N, 03Cr25Ni6Mo3Cu2N, UNS 32550 (Alloy255), wdg.

 

Ngwakọta kemịkalụ nke igwe weld (%):

C

Mn

Si

Cr

Ni

Mo

Cu

N

S

P

≤0.06

0.5-1.5

≤1.0

24.0 ~ 27.0

6.5-8.5

2.9-3.9

1.5-2.5

0.10 ~ 0,25

≤0.030

≤0.040

 

Njirimara nke igwe weld metal:

Nwalee ihe

Ike ọdụdọ

Mpa

Ogologo oge

%

Ekwenyere

≥760

≥15

 

Akwadoro ugbu a:

Dayameta mkpanaka

(mm)

2.5

3.2

4.0

5.0

Welding Ugbu a

(A)

50 ~ 80

80 ~ 110

110 ~ 160

160 ~ 200

 

Mara:

1. The electrode ga-abụọ maka 1 hour na gburugburu 250 ℃ tupu ịgbado ọkụ ọrụ;

2. Jiri ike ọkụ DC mee ihe dị ka o kwere mee, na ugbu a ekwesịghị ịdị ukwuu ka ọ ghara ịcha ọbara ọbara nke mkpanaka ịgbado ọkụ;

3. Tupu ịgbado ọkụ, wepụ mmanụ, nchara, ọnụ ọgụgụ, mmiri na adịghị ọcha ndị ọzọ n'elu akụkụ nke ịgbado ọkụ.

 

 

Wenzhou Tianyu Electronic Co., Ltd. e guzobere na 2000. Anyị na-etinye aka na n'ichepụta nkewelding electrodes, mkpanaka ịgbado ọkụ, nawelding consumablesihe karịrị afọ iri abụọ.

Isi ngwaahịa anyị gụnyere igwe anaghị agba ncharawelding electrodes, carbon ígwè ịgbado ọkụ electrodes, ala alloy ịgbado ọkụ electrodes, surfacing ịgbado ọkụ electrodes, nickel & cobalt alloy ịgbado ọkụ electrodes, nwayọọ ígwè & ala alloy ịgbado ọkụ wires, igwe anaghị agba nchara ịgbado ọkụ wires, gas-shielded flux cored wires, aluminum ịgbado ọkụ wires, submerged arc ịgbado ọkụ .wires, nickel & cobalt alloy welding wires, brass welding wires, TIG & MIG welding wires, tungsten electrodes, carbon gouging electrodes, na ndị ọzọ ịgbado ọkụ ngwa & consumables.

 

 