Nickel Alloy Welding Waya ERNiCr-3 Nickel Tig Wire Filler Metal

Nkọwa dị mkpirikpi:

Alloy 82 (ERNiCr-3) na-eji maka ịgbado ọkụ nke alloys 600, 601, 690, 800 na 800HT wdg.


Nkọwa ngwaahịa

Mkpado ngwaahịa

Nickel AlloyWaya ịgbado ọkụTig WayaERNiCr-3

Ụkpụrụ
TS EN ISO 18274 - Ni 6082 - NiCr20Mn3Nb
AWS A5.14 – ER NiCr-3

 

Atụmatụ na ngwa

Alloy 82 na-eji maka ịgbado ọkụ nke alloys 600, 601, 690, 800 na 800HT wdg.

Igwe weld etinyebere nwere ike dị elu yana ezigbo nguzogide corrosion, gụnyere nguzogide oxidation na ike mgbawa na-akpụ akpụ na okpomọkụ dị elu.

Kwesịrị ekwesị maka ngwa ịgbado ọkụ dị iche ichenickelalloys, igwe anaghị agba nchara, carbon steel gụnyere ihe mkpuchi.

Kwesịrị ekwesị maka ngwa sitere na cryogenic ruo na okpomọkụ dị elu na-eme ka alloy a bụrụ nke a na-ejikarị eme ihe na ezinụlọ nickel.

A na-ejikarị eme ihe na mmepụta ike na ụlọ ọrụ petrochemical wdg.

Ngwa ndị isi a na-ahụkarị

Alloy 600, Alloy 601, Alloy 690, Alloy 800, Alloy 330*
* Ihe atụ, ọ bụghị ndepụta zuru oke

 

 

Ngwakọta kemịkalụ%

C%

Mn%

Fe%

P%

S%

Si%

 

max

2.50

max

max

max

max

 

0.05

3.50

3.00

0,030

0.015

0,50

 

 

Cu%

Ni%

Co%

Ti%

kr%

Nb+Ta%

 

max

67.00

max

max

18.00

2.00

 

0,50

min

1.00

0.75

22.00

3.00

 

 

Ihe eji arụ ọrụ
Ike ọdụdọ ≥600 MPa  
Mpụta Ike ≥360 MPa  
Ogologo oge ≥30 MPa  
Mmetụta Mmetụta ≥100 MPa  

Ngwongwo eji arụ ọrụ dị ihe dị ka ma nwee ike ịdịgasị iche dabere na ọkụ, ikuku mkpuchi, paramita ịgbado ọkụ na ihe ndị ọzọ.

 

Gases na-echebe

TS EN ISO 14175 - TIG: I1 (Argon)

 

Ọnọdụ ịgbado ọkụ

TS EN ISO 6947-PA, PB, PC, PD, PE, PF, PG

 

Data nkwakọ
Dayameta Ogologo Ibu  
1.60 mm

2.40 mm

1000 mm

1000 mm

5 n'arọ

5 n'arọ

 

 