E310T1-1/4 FLUX-CORED WIRE

NKWUKWU
AWS 5.22 Klas E310T1-1/4 / ASME SFA A5.22 Klas E310T1-1/4
UNS W31031 A#9 F#6

Nkọwa
E310T1-1/4 bụ waya ikuku na-ekpuchi ikuku emebere maka ịgbado ọkụ “ọnọdụ niile” enwere ike iji ya na 75% Ar / 25% CO2 ma ọ bụ 100% CO2 gas.
A ga-emerịrị usoro ịgbado ọkụ ka ọ ghara ịgbawa ọkụ.

Ngwa
A na-ejikarị E310T1-1/4 eme ihe maka ịgbado agbado isi ọla nke ihe ndị yiri ya dị ka AISI 310 steels.
E310T1-1 / 4 nwere ike ji mee ihe maka ịgbado ọkụ carbon ígwè na igwe anaghị agba nchara.
E310T1-1/4 nwere ike iji maka ịgbado ọkụ ma ọ bụ rụkwaa elu alloy isi na corrosion eguzogide nkedo nke otu izugbe mejupụtara.
Jiri ntinye ọkụ dị obere - Tụọ 30,000 Joules/Kachasịa.
Zenarị chaplet weld concave
Debe okpomọkụ n'etiti 250ºF
Jupụta mmalite niile ma kwụsị olulu mmiri ka ịzenarị mgbawa ugwu.

CHINEKE NDỊ MMADỤ (%)

C Cr Ni Mo Mn Si P S Cu
.10 25.9 20.4 .10 1.4 .82 .015 .005 .08

Ngwongwo ndi oru

IKE ỌDỤDỌ 89,000 PSI
ỌTỤTỤ n'ime 2" 38%
Ọgwụgwọ okpomọkụ Ọ DỊGHỊ

Mara: Egosiputa ihe eji arụ ọrụ na-eji 100% CO2

NDỊ MMADỤ NDỊ MMADỤ NDỊ NA-ECHICHE (na-eji 100% CO2)

.045” DIA. FLAT & VERTICAL FLAT naanị
AMPS 130-190 120-250
VOLTS 24-29 25-29
WFS (IPM) 225-450 200-600

IHE: Wepụ 3/8"-1/2"
Obere volt site na 2 mgbe ị na-eji 75% Ar / 25% CO2

Wenzhou Tianyu Electronic Co., Ltd. e guzobere na 2000. Anyị na-etinye aka na n'ichepụta nke ịgbado ọkụ electrodes,mkpanaka ịgbado ọkụ, na welding consumables ihe karịrị afọ 20.

Ngwaahịa anyị bụ isi gụnyere igwe anaghị agba nchara igwe anaghị agba nchara, carbon steel ịgbado ọkụ electrodes, ala alloy ịgbado ọkụ electrodes, surfacing ịgbado ọkụ electrodes, nickel & cobalt alloy ịgbado ọkụ electrodes, nwayọọ ígwè & ala alloy ịgbado ọkụ wires, igwe anaghị agba nchara welding wires, gas-shielded flux cored wires, waya ịgbado ọkụ aluminom, ịgbado ọkụ n'okpuru mmiri.wires, nickel & cobalt alloy welding wires, brass welding wires, TIG & MIG welding wires, tungsten electrodes, carbon gouging electrodes, na ndị ọzọ ịgbado ọkụ ngwa & consumables.


  • Nke gara aga:
  • Osote: