E2209T1-1/T1-4 Igwe anaghị agba nchara Flux Cored Welding Waya

Nkọwa dị mkpirikpi:

A na-ahazi ya maka ịgbado ọkụ n'ọnọdụ, ma kwụ ọtọ na maka pipework a kapịrị ọnụ ruru eru na ọnọdụ ịgbado ọkụ ASME 5G ma ọ bụ 6G (ọkpọụ na-abụkarị> dayameta 150mm,> mgbidi 15mm).
Dị nro niile weldability ọnọdụ


Nkọwa ngwaahịa

Mkpado ngwaahịa

AWS Klas E2209T1-1/T1-4Flux Core Waya

Atụmatụ
A na-ahazi maka ịgbado ọkụ n'ọnọdụ, ma kwụ ọtọ na maka pipework a kapịrị ọnụ ruru eru na ọnọdụ ịgbado ọkụ ASME 5G ma ọ bụ 6G (ọkpọụ na-abụkarị> dayameta 150mm,> mgbidi 15mm).
Dị nro niile weldability ọnọdụ
Mwepụ slag dị mma

Gas na-echebe
80% argon / 20% CO2
100% CO2

Atụmatụ igodo
• Dị nro niile weldability ọnọdụ
• mkpọ mechiri emechi oghere
• Magburu onwe slag mwepụ
• Asambodo na-egosi nhazi nkwụnye ego, nọmba ferrite, na ihe mmetụta charpy anwalela @ -196°C (-320°F)

AWS Klas E2209T1-1/T1-4Flux Core WayaNgwakọta kemịkalụ

C Cr Ni Mo Mn Si P S N Cu
.03 22.5 9.7 3.25 0.95 .60 0.03 .015 0.14 0.20
AWS Klas E2209T1-1/T1-4 Flux Core Wire Mechanical Properties
Ike ọdụdọ 120,000 psi
Mpụta Ike 95,000 psi
Mgbatị (%) 26%
AWS Klas E2209T1-1/T1-4 Flux Core Wire Parameters
Dayameta WFS (ipm) Amperage Volt ESO (n'ime) Ọnụ ego nkwụnye ego
(lbs/hr)
.045" 250 130 22 5/8-3/4” 5.4
300 160 24 5/8-3/4” 6.3
425 200 26 5/8-3/4” 9.2
780 270 32 5/8-3/4” 16.2
1/16” 150 170 23 3/4-1” 5.4
195 215 25 3/4-1” 7.0
240 250 26 3/4-1” 8.6
320 305 27 3/4-1” 11.5

 

Wenzhou Tianyu Electronic Co., Ltd. e guzobere na 2000. Anyị na-etinye aka na n'ichepụta nke ịgbado ọkụ electrodes,mkpanaka ịgbado ọkụ, na welding consumables ihe karịrị afọ 20.

Ngwaahịa anyị bụ isi gụnyere igwe anaghị agba nchara igwe anaghị agba nchara, carbon steel ịgbado ọkụ electrodes, ala alloy ịgbado ọkụ electrodes, surfacing ịgbado ọkụ electrodes, nickel & cobalt alloy ịgbado ọkụ electrodes, nwayọọ ígwè & ala alloy ịgbado ọkụ wires, igwe anaghị agba nchara welding wires, gas-shielded flux cored wires, waya ịgbado ọkụ aluminom, ịgbado ọkụ n'okpuru mmiri.wires, nickel & cobalt alloy welding wires, brass welding wires, TIG & MIG welding wires, tungsten electrodes, carbon gouging electrodes, na ndị ọzọ ịgbado ọkụ ngwa & consumables.


  • Nke gara aga:
  • Osote: