E71T-11 Carbon Steel Flux Cored Arc Welding Electrodes Flux-Cored Welding Waya

Nkọwa dị mkpirikpi:

E71T-11 bụ a onwe-shielding flux cored waya eji maka ịgbado ọkụ carbon steels.


Nkọwa ngwaahịa

Mkpado ngwaahịa

E71T-11 A5.20, CARBON STEELFlux CoredArc Welding Electrodes

E71T-11 bụ a onwe-shielding flux cored waya eji maka ịgbado ọkụ carbon steels.Achọghị gas mkpuchi ma enwere ike iji ya rụọ ọrụ ịgbado ọkụ ọtụtụ ngafe.

Ngwa a na-ahụkarị: butt, lap and fillet welds na ígwè 16 nlele site na ½”;mgbakọ na mmezi ịgbado ọkụ;igwe akụkụ, tankị, prefab ewu

Klas AWS: E71T-11 Asambodo: AWS A5.20/A5.20M:2005
Alloy: E71T-11 AWS/ASME SFA A5.20

 

Ọnọdụ ịgbado ọkụ:
H, F, V-elu, O
Ugbu a:
DCEN

 

Ike tensile, kpsi: 70-95
Ike Mpụta, kpsi: 58 min
Mgbatị %: 20 min

Chemistry waya a na-ahụkarị dị ka AWS A5.9 (ụkpụrụ otu kacha)

C Mn Si S P Al  
0.30 1.75 0.60 0.03 0.03 1.80  
  Paramita waya a na-ahụkarị
Dayameta Ọnọdụ Usoro Amps Volt Ọsọ nri waya
in (mm)  
.030" 0.8 Ọnọdụ niile FCAW 25 14 55
    Ọnọdụ niile FCAW 125 16 225
.035" 0.9 Ọnọdụ niile FCAW 55 17 75
    Ọnọdụ niile FCAW 80 19 110
    Ọnọdụ niile FCAW 120 20 160
.045" 1.2 Ọnọdụ niile FCAW 115 15 105
    Ọnọdụ niile FCAW 130 16 125
    Ọnọdụ niile FCAW 160 17 170
    Ọnọdụ niile FCAW 200 18 195
1/6" 1.6 Ọnọdụ niile FCAW 160 17 70
    Ọnọdụ niile FCAW 190 18 100
    Flat & kwụ ọtọ FCAW 210 19 110
    Flat & kwụ ọtọ FCAW 260 20 145
0.068 1.7 Ọnọdụ niile FCAW 145 18 50
    Ọnọdụ niile FCAW 155 18 60
    Ọnọdụ niile FCAW 185 18 70
    Ọnọdụ niile FCAW 240 18 100
    Flat & kwụ ọtọ FCAW 255 21 111
    Flat & kwụ ọtọ FCAW 315 22 160
5/64 2.0 Ọnọdụ niile FCAW 185 16 55
    Ọnọdụ niile FCAW 190 18 60
    Ọnọdụ niile FCAW 220 19 70
    Flat & kwụ ọtọ FCAW 26 21 90
    Flat & kwụ ọtọ FCAW 315 22 124

 

 

Wenzhou Tianyu Electronic Co., Ltd. e guzobere na 2000. Anyị na-etinye aka na n'ichepụta nke ịgbado ọkụ electrodes,mkpanaka ịgbado ọkụ, na welding consumables ihe karịrị afọ 20.

Ngwaahịa anyị bụ isi gụnyere igwe anaghị agba nchara igwe anaghị agba nchara, carbon steel ịgbado ọkụ electrodes, ala alloy ịgbado ọkụ electrodes, surfacing ịgbado ọkụ electrodes, nickel & cobalt alloy ịgbado ọkụ electrodes, nwayọọ ígwè & ala alloy ịgbado ọkụ wires, igwe anaghị agba nchara welding wires, gas-shielded flux cored wires, waya ịgbado ọkụ aluminom, ịgbado ọkụ n'okpuru mmiri.wires, nickel & cobalt alloy welding wires, brass welding wires, TIG & MIG welding wires, tungsten electrodes, carbon gouging electrodes, na ndị ọzọ ịgbado ọkụ ngwa & consumables.


  • Nke gara aga:
  • Osote: