Flux Cored Arc Welding Wire AWS A5.22 E309LMoT1-1 igwe anaghị agba nchara.

Nkọwa dị mkpirikpi:

AWS A5.22 E309LMoT1-1 Flux Cored Arc Welding Wire bụ ụdị 309L gbanwere yana mgbakwunye molybdenum.


Nkọwa ngwaahịa

Mkpado ngwaahịa

Flux CoredArcWaya ịgbado ọkụ AWS A5.22 E309LMoT1-1

TS EN ISO 17633-AT23 12LPC1 1

Njirimara na ngwa
AWS A5.22 E309LMoT1-1 Flux Cored Arc Welding Wire bụ ụdị 309L gbanwere yana mgbakwunye molybdenum.Ọ bụ
dabara adaba maka ijikọ igwe anaghị agba nchara na igwe anaghị agba nchara.Mgbakwunye nke molybdenum na-eme ka ike na-akpụ akpụ na
na-eme ka nguzogide corrosion dịkwuo mma.

Ihe mejupụtara kemịkalụ nke igwe weld (%)
C 0.025 Mn1.16 Si0.57 P 0.023 S 0.007 Cr 23.46 Ni 12.51 Mo 2.20

Njirimara arụrụ arụ nke igwe Weld
Ike tensile 685MPa elongation 33%

Ihe edeturu maka ojiji:
1. Tupu ịgbado ọkụ, mmanụ, nchara, na mmiri kwesịrị ihicha na isi ihe kwesịrị inwe nke kwesịrị ekwesị.
nchebe site na ifufe na saịtị ịgbado ọkụ.
2. Jiri 99.8% ma ọ bụ elu dị ọcha Co2 dị ka ikpuchi gas.Wenzhou Tianyu Electronic Co., Ltd. e guzobere na 2000. Anyị na-etinye aka na n'ichepụta nke ịgbado ọkụ electrodes,mkpanaka ịgbado ọkụ, na welding consumables ihe karịrị afọ 20.

Ngwaahịa anyị bụ isi gụnyere igwe anaghị agba nchara igwe anaghị agba nchara, carbon steel ịgbado ọkụ electrodes, ala alloy ịgbado ọkụ electrodes, surfacing ịgbado ọkụ electrodes, nickel & cobalt alloy ịgbado ọkụ electrodes, nwayọọ ígwè & ala alloy ịgbado ọkụ wires, igwe anaghị agba nchara welding wires, gas-shielded flux cored wires, waya ịgbado ọkụ aluminom, ịgbado ọkụ n'okpuru mmiri.wires, nickel & cobalt alloy welding wires, brass welding wires, TIG & MIG welding wires, tungsten electrodes, carbon gouging electrodes, na ndị ọzọ ịgbado ọkụ ngwa & consumables.