AF2209-15 (AWS E2209-15) Igwe anaghị agba nchara Electrode nwere mkpuchi hydrogen dị ala.Mkpara maka ịgbado ọkụ

Nkọwa dị mkpirikpi:

AF2209-15 (AWS E2209-15) bụ obere carbon nitrogen nwere duplex igwe anaghị agba nchara nwere mkpuchi hydrogen dị ala.


Nkọwa ngwaahịa

Mkpado ngwaahịa

Igwe anaghị agba ncharaElectrode

AF2209-15

GB/T E2209-15

AWS A5.4 E2209-15

Nkọwa: AF2209-15 bụ obere carbon nitrogen nwere duplex igwe anaghị agba nchara nwere mkpuchi hydrogen dị ala.Jiri DCEP (ezigbo electrode ugbu a kpọmkwem).Ịrụ ọrụ dị oke mma.N'ihi na ọ nwere molybdenum na nitrogen, na carbon ọdịnaya dị oke ala, metal ahụ etinyere nwere ezigbo nguzogide mgbape na nguzogide corrosion, karịsịa nrụgide corrosion nguzogide.

Ngwa: A na-eji ya eme ihe maka ịgbado ọkụ otu ụdị ihe igwe anaghị agba nchara ultra-low na mmanụ ala na ụlọ ọrụ hydraulic.Dị ka ịgbado ọkụ nke 022Cr22Ni5Mo3N duplex igwe anaghị agba nchara.

 

Ngwakọta kemịkalụ nke igwe weld (%):

C

Mn

Si

Cr

Ni

Mo

N

Cu

S

P

≤0.04

0.5-2.0

≤0.90

21.5 ~ 23.5

8.5 ~ 10.5

2.5-3.5

0.08 ~ 0,20

≤0.75

≤0.030

≤0.040

 

Njirimara nke igwe weld metal:

Nwalee ihe

Ike ọdụdọ

Mpa

Ogologo oge

%

Ekwenyere

≥690

≥20

 

Akwadoro ugbu a:

Dayameta mkpanaka

(mm)

2.5

3.2

4.0

5.0

Welding Ugbu a

(A)

50 ~ 70

80 ~ 110

130 ~ 150

160 ~ 200

 

Mara:

1. The electrode ga-abụọ maka 1 hour na gburugburu 250 ℃ tupu ịgbado ọkụ ọrụ;

2. Ọ dị mkpa iji kpochaa nchara, ọnụ ọgụgụ mmanụ, mmiri na adịghị ọcha na akụkụ ịgbado ọkụ tupu ịgbado ọkụ.

 

 

Wenzhou Tianyu Electronic Co., Ltd. e guzobere na 2000. Anyị na-etinye aka na n'ichepụta nkewelding electrodes, mkpanaka ịgbado ọkụ, nawelding consumablesihe karịrị afọ iri abụọ.

Ngwaahịa anyị bụ isi gụnyere igwe anaghị agba nchara igwe anaghị agba nchara, carbon steel ịgbado ọkụ electrodes, ala alloy ịgbado ọkụ electrodes, surfacing ịgbado ọkụ electrodes, nickel & cobalt alloy ịgbado ọkụ electrodes, nwayọọ ígwè & ala alloy ịgbado ọkụ wires, igwe anaghị agba nchara welding wires, gas-shielded flux cored wires, waya ịgbado ọkụ aluminom, ịgbado ọkụ n'okpuru mmiri.wires, nickel & cobalt alloy welding wires, brass welding wires, TIG & MIG welding wires, tungsten electrodes, carbon gouging electrodes, na ndị ọzọ ịgbado ọkụ ngwa & consumables.

 

 


  • Nke gara aga:
  • Osote: