Elektrọd ígwè hydrogen carbon dị ala E6011

Nkọwa Dị Mkpirikpi:

AWS E6011elektrọd ịgbado ọkụbụ ụdị potassium cellulose, nke a na-eji maka ịgbado ọkụ kwụ ọtọ. Ma maka ịgbado ọkụ AC na DC.


Nkọwa Ngwaahịa

Akara Ngwaahịa

Ngwa
Mkpanaka ịgbado ọkụ AWS E6011 Ọ dabara adaba maka nhazi arịa ịgbado ọkụ dịka ụlọ na àkwà mmiri, tankị nchekwa, ọkpọkọ na ihe ndị metụtara arịa nrụgide.

AWS E6011elektrọd ịgbado ọkụbụ ụdị potassium cellulose, nke a na-eji maka ịgbado ọkụ kwụ ọtọ. Ma maka ịgbado ọkụ AC na DC. Ọ na-anabata teknụzụ mba ọzọ dị elu ma nwee nnukwu ihe ọmụma teknụzụ ịgbado ọkụ. Ogologo ARC kwesịrị ịdị n'ókè kwesịrị ekwesị. Ọ bụghị ịgbado ọkụ na mkpuchi mkpuchi kwesịrị ekwesị.

Ihe mejupụtara kemịkalụ (%)
C Mn Si S P
≤0.2 0.3-0.6 ≤0.22 ≤0.03 ≤0.04
Njirimara Mechanical nke Metal E tinyere n'ime ya
Ihe Nnwale Rm (N/mm2) Rel (N/mm2) A (%) KV2(J) 0℃
Uru nkwa ≥420 ≥330 ≥22 ≥47
Nsonaazụ Izugbe 485 380 24 86
Ugbu a (DC)
Dayameta φ2.0 φ2.5 φ3.2 φ4.0 φ5.0
Ampereji 40 ~ 70 50 ~ 90 90 ~ 130 130 ~ 210 170 ~ 230

ỤDỊ ỌRỤ: Electrode ỌRỤ ỌRỤ Direct (DCEP) ma ọ bụ AC

Usoro ịgbado ọkụ akwadoro:

Ogologo Arc - Ogologo nkezi (1/8" ruo 1/4")

Dị larịị - Gaa n'ihu ọdọ mmiri ma jiri obere mmegharị ịkụ ihe

Kwụ ọtọ - Elektrọd akụkụ ntakịrị na-aga n'elu efere

Elu kwụ ọtọ - obere usoro ịkụ ihe ma ọ bụ ịkpa ákwà

Ala kwụ ọtọ - Jiri amperage dị elu ma gaa ngwa ngwa, na-anọ n'ihu ọdọ mmiri

Overhead - Gaa n'ihu ọdọ mmiri ma jiri obere mmegharị ịkụ ihe

Nlebara anya:
1. Ọ dị mfe ikpughe ya na mmiri, biko debe ya n'ọnọdụ kpọrọ nkụ.
2. Ọ chọrọ ikpo ọkụ mgbe ngwugwu gbawara ma ọ bụ mmiri batara, okpomọkụ ikpo ọkụ kwesịrị ịdị n'etiti 70C ruo 80C, oge ikpo ọkụ kwesịrị ịdị site na 0.5 ruo 1 awa.
3. Mgbe ị na-eji elektrọd ịgbado ọkụ nke 5.0mm, ọ ka mma iji ike dị elu, nke na-ebelata ọkụ eletrik, iji mee ka arụmọrụ ịgbado ọkụ dịkwuo mma.

  • Nke gara aga:
  • Osote: