Mkpanaka ịgbado ọkụ nke ígwè carbon E7018

Nkọwa Dị Mkpirikpi:

Mkpanaka ịgbado ọkụ AWS E7018 bụ elektrọd ígwè carbon nke nwere obere hydrogen iron potassium kpuchie.


Nkọwa Ngwaahịa

Akara Ngwaahịa

Nhazi:

AWS A5.1 E7018

ISO 2560-B-E4918A

GB/T 5117 E5018

Mkpanaka ịgbado ọkụ AWS E7018 bụ elektrọd ígwè carbon nke nwere obere hydrogen iron potassium powder covered. Uzuzu ígwè dị na mkpuchi ahụ na-eme ka ọnụego nkwụnye ego dịkwuo elu. O nwere ezigbo ojiji nke na-enye ya ohere inwe arc kwụsiri ike, obere splatter, iwepụ slag dị mfe ma na-agbakọta n'ọnọdụ niile. Ígwè e tinyere na ya nwere ezigbo ihe eji arụ ọrụ nke na-enye ezigbo ike okpomọkụ dị ala.

Mkpanaka ịgbado ọkụ AWS E7018 (electrode ntụ ntụ ígwè bụ isi) dabara adaba maka ịgbado ọkụ nke ígwè carbon na usoro ígwè alloy dị ala, dịka Gr.50, wdg.

Ihe mejupụtara kemịkalụ (%)
Ngwakọta Kemịkalụ

C

Mn

Si

S

P

Uru nkwa

≤0.12

≤1.60

≤0.75

≤0.035

≤0.040

Nsonaazụ Izugbe

0.089

1.2

0.38

0.028

0.04

Njirimara mekaniki nke ígwè e tinyere ego
Ihe Nnwale

Rm (N/mm2)

Rel (N/mm2)

A (%)

KV2(J) -30°C

Uru nkwa

≥490

≥400

≥20

≥27

Nsonaazụ Izugbe

515

430

32

156

Ọsọ ntụaka (DC)

Dayameta

φ2.5

φ3.2

φ4.0

φ5.0

Ampereji

60 ~ 100

80 ~ 140

110 ~ 210

160 ~ 230

Nnyocha redio X-ray: ỌkwaⅠ

Ọnọdụ ịgbado ọkụ:

PA, PB, PC, PD, PE, PF

Ihe ndị e dere:
1. A ga-ekpo ọkụ elektrọd ahụ n'ọkụ n'okpomọkụ nke 350°C ruo otu awa. Kpoo mkpanaka ahụ ọkụ mgbe ọ bụla ejiri ya.
2. A ga-ehichapụ ihe ndị na-adịghị ọcha dịka nchara, ntụpọ mmanụ na mmiri n'ebe a na-arụ ọrụ.
3. A chọrọ obere arc iji rụọ ọrụ ịgbado ọkụ. Ụzọ ịgbado ọkụ dị warara ka mma.