J501Fe13 (AWS E7028) bụ carbon ígwè electrode na ígwè ntụ ntụ na obere hydrogen potassium mkpuchi.


Nkọwa ngwaahịa

Mkpado ngwaahịa

Carbon Steel Welding Electrode

J506Fe13

GB/T E5028

AWS A5.1 E7028

Nkọwa: J501Fe13 bụ carbon ígwè electrode na ígwè ntụ ntụ na obere hydrogen potassium mkpuchi.AC na DC bụ ebumnuche abụọ, dabara adaba maka ịgbado ọkụ dị larịị na ịgbado ọkụ dị larịị.Ịrụ ọrụ nkwụnye ego dị ihe dịka 130%.

Ngwa: Ọ na-eji ewepụghị ịgbado ọkụ na ewepụghị n'akuku ịgbado ọkụ nke carbon ígwè na ala alloy ígwè, dị ka Q345, wdg

 

Ngwakọta kemịkalụ nke igwe weld (%):

C

Mn

Si

S

P

≤0.12

≤1.60

≤0.75

≤0.035

≤0.035

 

Njirimara nke igwe weld metal:

Nwalee ihe

Ike ọdụdọ

Mpa

Mpụta ike

Mpa

Ogologo oge

%

Uru mmetụta (J)

(-46 ℃)

Ekwenyere

≥490

≥400

≥22

≥27

 

Ọdịnaya mgbasa hydrogen nke ọla edobere: ≤8.0mL/100g (usoro glycerin)

 

Nyocha X-ray: II ọkwa

 

Akwadoro ugbu a:

Dayameta mkpanaka

(mm)

4.0

5.0

Welding ugbu a

(A)

180 ~ 220

210 ~ 260

 

Mara:

1.The electrode ga-eme achịcha maka 1 hour na 350 ℃ tupu ịgbado ọkụ ọrụ;

2. Ọ dị mkpa iji kpochaa nchara, ọnụ ọgụgụ mmanụ, mmiri na adịghị ọcha na akụkụ ịgbado ọkụ tupu ịgbado ọkụ.

 

Wenzhou Tianyu Electronic Co., Ltd. e guzobere na 2000. Anyị na-etinye aka na mmepụta nke electrodes ịgbado ọkụ, mkpara ịgbado ọkụ, na ịgbado ọkụ consumables n'ihi na ihe karịrị 20 afọ.

Ngwaahịa anyị bụ isi gụnyere igwe anaghị agba nchara igwe anaghị agba nchara, carbon steel ịgbado ọkụ electrodes, ala alloy ịgbado ọkụ electrodes, surfacing ịgbado ọkụ electrodes, nickel & cobalt alloy ịgbado ọkụ electrodes, nwayọọ ígwè & ala alloy ịgbado ọkụ wires, igwe anaghị agba nchara welding wires, gas-shielded flux cored wires, waya ịgbado ọkụ aluminom, ịgbado ọkụ n'okpuru mmiri.wires, nickel & cobalt alloy welding wires, brass welding wires, TIG & MIG welding wires, tungsten electrodes, carbon gouging electrodes, na ndị ọzọ ịgbado ọkụ ngwa & consumables.

 


  • Nke gara aga:
  • Osote: