E6010 ihe eji ejikọ elektrọd ígwè carbon

Nkọwa Dị Mkpirikpi:

E6010 bụ electrode nke ụdị sodium rutile-cellulosic.


Nkọwa Ngwaahịa

Akara Ngwaahịa

AWS E6010 Electrode Ịgbado Ọkụ Dị Mfe

Ngwa:

Ọ dabara adaba maka ịgbado ọkụ nke obere usoro ígwè carbon dị ka pipeline, iwu ụgbọ mmiri na akwa mmiri wdg.

NKỌWA:

AWS A5.1 / ASME SFA5.1 E6010

JIS Z3211 D4310

ÀGWÀ:

E6010 bụ elektrọd sodium rutile-cellulosic. Enwere ike ịgbado ya maka ọnọdụ niile (karịsịa maka ọnọdụ kwụ ọtọ-ala) naanị site na DC+. Ọ nwere arụmọrụ ịgbado ya dị mma dịka arc kwụsiri ike, obere splatter, iwepụ slag dị mfe na ikike ịchịgharị wdg. Njikwa ọdọ mmiri gbazere agbaze ka mma, ike arc siri ike na ntinye miri emi na ọnọdụ kwụ ọtọ-ala.

MMIRI KEMIKỌTA NKE Ígwè NKỌWA NILE: (Mba %)

ihe C Mn Si S P Ni Cr Mo V
Ihe achọrọ ≤0.20 0.3-0.6 ≤0.30 ≤0.035 ≤0.040 ≤0.30 ≤0.20 ≤0.30 ≤0.08
Nsonaazụ Ndị A Na-ahụkarị 0.09 0.48 0.23 0.020 0.025 0.030 0.035 0.005 0.004

Njirimara MEKANỊKỤ NKE Ígwè WELD NILE:

ihe Rm/MPa Rel/Rp0.2 /MPa A/% KV2 (-30℃) /J
Ihe achọrọ ≥430 ≥330 ≥20 ≥27
Nsonaazụ Ndị A Na-ahụkarị 475 narị anọ 26 80

Ntị:

1. N'ozuzu, ọ dịghị mkpa ka e kpoo elektrọd ahụ ọzọ tupu e jiri ya gbaa ya ọkụ. Ọ bụrụ na mmiri dị n'ime ya emetụ ya, a ga-akpọghachi ya ọkụ na 70℃-90℃ ruo otu awa.

2. A ga-ewepụ nchara, mmanụ, mmiri na ihe ndị ọzọ na-adịghị mma nke ebe a na-agbakọta ihe tupu a na-agbakọta ihe.

Usoro Ọrụ A Na-ahụkarị: (DC+)

Dayameta (mm) 2.5 3.2 4.0 5.0
Ogologo (mm) 300 350 narị anọ narị anọ
Ugbu a (A) Afọ 50-80 60-100 100-140 140-180

NKWEKỌTA:

5kg/igbe, igbe 4/katọn, 20kgs/katọn, 50 katọn/pallet. 21MT -26MT kwa 1X20″ FCL.

 

OEM/ODM:

Anyị na-akwado OEM/ODM ma nwee ike ime nkwakọ ngwaahịa dịka imewe gị si dị, biko kpọtụrụ anyị maka mkparịta ụka zuru ezu.

 

Njirimara na Ojiji:

Nkịtị kwụsiri ike nke ukwuu.

Mwepụ dị mma nke slag.

Ntinye aka dị obere.

Ezigbo iguzogide okpomọkụ na nchara.

Nnukwu iguzogide mgbawa.


  • Nke gara aga:
  • Osote: