Electrọd ịgbado ọkụ E410NiMo-15

Nkọwa Dị Mkpirikpi:

E410NiMo-15 bụ elektrọd igwe anaghị agba nchara nke a na-akpọ martensitic, nke nwere obere hydrogen sodium mkpuchi, nke dị 11.0-12.5% ​​Cr, 4.0-5.0 Ni, na 0.40-0.70% Mo.


Nkọwa Ngwaahịa

Akara Ngwaahịa

Ụkpụrụ kwekọrọ

GB/T 983-2012 E410NiMo-15

AWS A5.4M-2012 E410NiMo-15

Ihe Dakọtara:1.4317 GX4CrNi13-4,1.4313 X3CrNiMo13-4,1.4407 GX5CrNiMo13-4,1.4414 GX4CrNiMo13-4,ACI Gr. CA6NM, UNS S41500

Nkọwa

E410NiMo-15 bụ elektrọd igwe anaghị agba nchara nke a na-akpọ martensitic nke nwere obere mkpuchi sodium hydrogen, nke nwere 11.0-12.5% ​​Cr, 4.0-5.0% Ni, na 0.40-0.70% Mo. Ọ dabara maka ịgbado ọkụ metal arc nke a na-echebe n'ọnọdụ niile (SMAW) nke nwere arc kwụsiri ike, obere splatter, na ezigbo slag nke a na-ewepụ. Ígwè a na-etinye na ya na-enye ike dị elu, ezigbo iguzogide nchara, na iguzogide mgbawa. A na-atụ aro ka a kpoo ọkụ tupu oge eruo maka ọrụ dị arọ, a na-achọkwa ọgwụgwọ okpomọkụ mgbe weld gasịrị (PWHT) na 580 ~ 620℃ (awa 1-2, ikuku oyi, AC).

Ngwa

Ọ dị mma maka ịgbado ígwè ASTM CA6NM, ígwè 13%Cr-4%Ni (dịka ọmụmaatụ, Cr13Ni4Mo, Cr13Ni5Mo), na ígwè igwe anaghị agba nchara yiri ya. A na-ejikarị ya arụ ọrụ dịka ịgbado ọkụ nke ndị na-agbagharị turbine ike mmiri, ahụ valvụ, paịpụ ndị nwere nrụgide dị elu, na elu nke ihe ndị e ji cavitation kpuchie. A na-ejikwa ya arụzi akụkụ ndị na-anaghị emebi emebi dịka mpịakọta crusher na ihe mkpuchi ọkpọkọ.

Ngwakọta Kemịkalụ nke Weld Metal(%)

Ihe C Mn Si P S Cr Ni Mo Cu
Ihe achọrọ ≤0.06 ≤1.0 ≤0.90 ≤0.04 ≤0.03 11.0-12.5 4.0-5.0 0.40-0.70 ≤0.75
Nsonaazụ Ule 0.029 0.7 0.32 0.028 0.01 12.26 4.50 0.55 0.01

Njirimara Mechanical nke Metal E tinyere n'ime ya

Aha Ule Ike nrụgide (Mpa) Ogologo% X-Ray Nnwale Mmetụta,(+20℃)J Ike HB Haịdọn A Na-agbasa (ml/100g)
Ihe achọrọ ≥760 ≥15 Ọkwa nke Mbụ – – ≤5
Nsonaazụ Ule 845 19 Ọkwa nke Mbụ 60-90 250-310 ≤5

Usoro ịgbado ọkụ akwadoro

Isi Iyi Ike: DC Reserve (DC-)

Ugbu a akwadoro

Dayameta mkpanaka (mm) 3.2 4.0 5.0
Ọsọ ịgbado ọkụ (A) 80-120 120-160 150-190

Rịba ama:

1. Mee ka elektrọd ahụ sie ike ruo awa 300 tupu ejiri ya wepụ mmiri mmiri.
2. Hichaa nchara, mmanụ, na mmiri site na elu ígwè dị n'okpuru ya; jiri obere ọrụ maka obere ihe e ji agwakọta ihe.
3. A ga-arụ PWHT ozugbo agbachara ya iji zere mmebi.

  • Nke gara aga:
  • Osote: