Tyue Brand Best Welding Electrodes AWS A5.4 E320-16 maka igwe anaghị agba nchara.

Nkọwa dị mkpirikpi:

A902 (AWS E320-16) bụ igwe anaghị agba nchara electrode nwere titanium-calcium mkpuchi.Enwere ike iji ya maka ma AC na DC na arụmọrụ arụmọrụ dị mma.


Nkọwa ngwaahịa

Mkpado ngwaahịa

Igwe anaghị agba ncharaElectrode

A902

GB/T E320-16

AWS A5.4 E320-16

Nkọwa: A902 bụ igwe anaghị agba nchara na mkpuchi titanium-calcium.Enwere ike iji ya maka ma AC na DC na arụmọrụ arụmọrụ dị mma.Ngwongwo etinyere ya nwere ezigbo nguzogide corrosion na nguzogide oxidation siri ike ma na-eji ya eme ihe n'imepụta ụlọ ọrụ kemịkalụ, mmanụ ala, na akụrụngwa mmepụta hydrogen.

Ngwa: Eji maka ịgbado ọkụ nke Carpenter20Cb nickel alloy na sulfuric acid, nitric acid, phosphoric acid na oxidative acid corrosion media.Enwere ike iji ya maka ịgbado ígwè dị iche iche.

 

Ngwakọta kemịkalụ nke igwe weld (%):

C

Si

Mn

Cr

Ni

Mo

Cu

Nb

S

P

≤0.07

≤0.60

0.5-2.5

19.0 ~ 21.0

32.0 ~ 36.0

2.0 ~ 3.0

3.0 ~ 4.0

8 XC ~ 1.00

≤0.030

≤0.030

 

Njirimara nke igwe weld metal:

Nwalee ihe

 Ike ọdụdọ

Mpa

Ogologo oge

%

Ekwenyere

≥550

≥30

 

Akwadoro ugbu a:

Dayameta mkpanaka

(mm)

2.5

3.2

4.0

Welding Ugbu a

(A)

50 ~ 80

80 ~ 110

110 ~ 160

 

Mara:

  1. The electrode ga-abụọ maka 1 hour na gburugburu 150 ℃ tupu ịgbado ọkụ ọrụ;
  2. N'ihi na omimi ntinye adịghị omimi n'oge ịgbado ọkụ AC, a ga-eji ọkụ ọkụ DC mee ihe dịka o kwere mee iji nweta ntinye miri emi.na nke ugbu a ekwesịghị ịbụ oke buru ibu iji zere ịcha ọbara ọbara nke mkpanaka ịgbado ọkụ.

 

 

Wenzhou Tianyu Electronic Co., Ltd. e guzobere na 2000. Anyị na-etinye aka na n'ichepụta nkewelding electrodes, mkpanaka ịgbado ọkụ, nawelding consumablesihe karịrị afọ iri abụọ.

Isi ngwaahịa anyị gụnyere igwe anaghị agba ncharawelding electrodes, carbon ígwè ịgbado ọkụ electrodes, ala alloy ịgbado ọkụ electrodes, surfacing ịgbado ọkụ electrodes, nickel & cobalt alloy ịgbado ọkụ electrodes, nwayọọ ígwè & ala alloy ịgbado ọkụ wires, igwe anaghị agba nchara ịgbado ọkụ wires, gas-shielded flux cored wires, aluminum ịgbado ọkụ wires, submerged arc ịgbado ọkụ .wires, nickel & cobalt alloy welding wires, brass welding wires, TIG & MIG welding wires, tungsten electrodes, carbon gouging electrodes, na ndị ọzọ ịgbado ọkụ ngwa & consumables.

 