GB/T EZNiCu-1 (Z508) Nkedo iron ịgbado ọkụ electrode Nickel-ọla kọpa Alloy (Monel) isi na eserese eserese.

Nkọwa dị mkpirikpi:

GB/T EZNiCu-1 (Z508) bụ ihe nkedo ígwè ịgbado ọkụ electrode nwere nickel-ọla kọpa alloy (Monel) isi na a graphitized mkpuchi.


Nkọwa ngwaahịa

Mkpado ngwaahịa

Nkedo ígwè ịgbado ọkụElectrode

Z508                                                     

GB/T EZNiCu-1

Nkọwa: Z508 bụ igwe ịgbado ọkụ nkedo nke nwere isi nickel-ọla kọpa (Monel) yana mkpuchi graphitized.AC na DC dual-nzube, arc kwụsiri ike, dị mfe iji rụọ ọrụ.Nrụpụta ya na ịrụ ọrụ ịkpụ ya dị nso na Z308, mana n'ihi nnukwu mbelata nke ọla edobere, nguzogide mgbape adịghị mma.Ike nke nkwonkwo welded dị ala, n'ihi ya, ọ dịghị mma maka ịgbado ọkụ nke akụkụ ndị nwere nrụgide.

Ngwa: A na-eji ya maka ịgbado ọkụ nrụzi nke nkedo isi awọ nke na-achọghị ike dị elu.

 

Ngwakọta kemịkalụ nke igwe weld (%):

C

Si

Mn

Fe

S

Ni

Cu

Ndị ọzọ

0,35 ~ 0,55

≤0.75

≤2.3

3.0 ~ 6.0

≤0.025

60 ~ 70

25-35

≤1.0

 

Akwadoro ugbu a:

Dayameta mkpanaka

(mm)

3.2

4.0

5.0

Welding ugbu a

(A)

90 ~ 110

120 ~ 150

160 ~ 190

 

Mara:

1. The electrode ga-n'ihi na 1 hour gburugburu 150 ℃ tupu ịgbado ọkụ ọrụ;

2. Mgbe ị na-agbado ọkụ, ọ bụ ihe amamihe dị na ya iji ụzọ dị warara, na ogologo nke weld ọ bụla ekwesịghị gafere 50mm.Ngwa ngwa were obere hama jikwaa weld ahụ iji belata nrụgide na mpaghara nrụzi weld wee gbochie mgbawa mgbe ịgbadochara ọkụ.

 

 

Wenzhou Tianyu Electronic Co., Ltd. e hiwere na 2000. Anyị na-etinye aka na n'ichepụta nke ịgbado ọkụ electrodes, ịgbado ọkụ mkpara, naịgbado ọkụ ọkụs maka ihe karịrị afọ 20.

Ngwaahịa anyị bụ isi gụnyere igwe anaghị agba nchara igwe anaghị agba nchara, carbon steel ịgbado ọkụ electrodes, ala alloy ịgbado ọkụ electrodes, surfacing ịgbado ọkụ electrodes, nickel & cobalt alloy ịgbado ọkụ electrodes, nwayọọ ígwè & ala alloy ịgbado ọkụ wires, igwe anaghị agba nchara welding wires, gas-shielded flux cored wires, waya ịgbado ọkụ aluminom, ịgbado ọkụ n'okpuru mmiri.wires, nickel & cobalt alloy welding wires, brass welding wires, TIG & MIG welding wires, tungsten electrodes, carbon gouging electrodes, na ndị ọzọ ịgbado ọkụ ngwa & consumables.

 


  • Nke gara aga:
  • Osote: