AWS A5.11 ENiCrFe-9 Nickel na Nickel Alloy Welding Electrodes, Akwụkwọ ntuziaka Metal Arc Electrodes, mkpanaka ịgbado ọkụ

Nkọwa dị mkpirikpi:

Ni327 (AWS ENiCrFe-9) bụ electrode dabere na nickel nwere mkpuchi sodium dị ala.Jiri DCEP (ezigbo electrode ugbu a kpọmkwem).


Nkọwa ngwaahịa

Mkpado ngwaahịa

Nickel na Nickel Alloy Welding Electrode

Ni327                                                     

GB/T ENi6094

AWS A5.11 ENiCrFe-9

Nkọwa: Ni327 bụ electrode dabeere na nickel nwere mkpuchi sodium dị ala.Jiri DCEP (electrode ugbu a kpọmkwemnti).Igwe a na-echekwara nwere ezigbo nguzogide mgbape n'ihi na weld nwere ụfọdụ ihe na-eme ka ihe dị ka molybdenum na niobium.

Ngwa: A na-eji ya maka ịgbado ọkụ nickel alloys nke chọrọ nguzogide okpomọkụ na nguzogide corrosion, a pụkwara iji ya mee ihe maka ịgbado ọkụ na surfacing nke ụfọdụ alloys siri ike na-weld na nchara dị iche iche.

 

Ngwakọta kemịkalụ nke igwe weld (%):

C

Mn

Fe

Si

Cu

Ni

Cr

≤0.15

1.0-4.5

≤12.0

≤0.8

≤0.5

≥55.0

12.0 ~ 17.0

Nb + Ta

Mo

W

S

P

Ndị ọzọ

 

0.5-3.0

2.5-5.5

≤1.5

≤0.015

≤0.020

≤0.50

 

 

Njirimara nke igwe weld metal:

Nwalee ihe

Ike ọdụdọ

Mpa

Mpụta ike

Mpa

Ogologo oge

%

Ekwenyere

≥650

≥360

≥18

 

Akwadoro ugbu a:

Dayameta mkpanaka

(mm)

3.2

4.0

Welding ugbu a

(A)

90 ~ 110

110 ~ 150

 

Mara:

1. The electrode ga-abụọ maka 1 hour na gburugburu 300 ℃ tupu ịgbado ọkụ ọrụ;

2. Ọ dị mkpa iji kpochaa nchara, mmanụ, mmiri na adịghị ọcha na akụkụ ịgbado ọkụ tupu ịgbado ọkụ.

 