Mgbado ọkụ AWS A5.11 ENiCrFe-3 Nickel Dabere Alloy Welding Electrodes, Nickel Arc Welding Rods

Nkọwa dị mkpirikpi:

Ni307-3 (AWS ENiCrFe-3) bụ electrode dabeere na nickel nke nwere mkpuchi sodium dị ala.Jiri DCEP (ezigbo electrode ugbu a kpọmkwem).


Nkọwa ngwaahịa

Mkpado ngwaahịa

Nickel na Nickel Alloy Welding Electrode

Ni307-3                                                     

GB/T ENi6182

AWS A5.11 ENiCrFe-3

Nkọwa: Ni307-3 bụ anickel-dabere na electrode na obere-hydrogen sodium mkpuchi.Jiri DCEP (ezigbo electrode ugbu a kpọmkwem).Ọ nwere ezigbo mgbape mgbape n'ihi na weld nwere ụfọdụ manganese, niobium, na ihe ndị ọzọ na-eme ka ihe ndị ọzọ na-eme ihe.

Ngwa: Ọ na-eji maka ịgbado ọkụ nkenickel-chromium-iron alloys (dị ka UNS N06600) na nchara nke nchara.Ọnọdụ okpomọkụ na-arụ ọrụ adịghị elu karịa 480 Celsius C, na nkwụsị mgbape dị mma.Kwesịrị ekwesị maka ụgbọ mmiri nrụgide ọkụ atomiki na ịgbado ọkụ tankị kemịkal.

 

Ngwakọta kemịkalụ nke igwe weld (%):

C

Mn

Fe

P

S

Si

Cu

≤0.10

5.0 ~ 10.0

≤10.0

≤0.020

≤0.015

≤1.0

≤0.5

Ni

Ti

Mo

Nb

Ta

Ndị ọzọ

 

≥60.0

≤1.0

13.0 ~ 17.0

1.0-3.5

≤0.30

≤0.50

 

 

Njirimara nke igwe weld metal:

Nwalee ihe

Ike ọdụdọ

Mpa

Mpụta ike

Mpa

Ogologo oge

%

Ekwenyere

≥550

≥360

≥27

 

Akwadoro ugbu a:

Dayameta mkpanaka

(mm)

2.5

3.2

4.0

5.0

Welding ugbu a

(A)

60 ~ 90

80 ~ 100

110 ~ 150

130 ~ 180

 

Mara:

1. The electrode ga-abụọ maka 1 hour na gburugburu 300 ℃ tupu ịgbado ọkụ ọrụ;

2. Ọ dị mkpa iji kpochaa nchara, mmanụ, mmiri na adịghị ọcha na akụkụ ịgbado ọkụ tupu ịgbado ọkụ.Gbalịa iji obere arc iji weld.

 