TYUE E6013(J421X) ELECTRODE Ígwè KABỌN

Nkọwa Dị Mkpirikpi:

AWS A5.1 E6013(J421) bụ elektrọd ụdị rutile.


Nkọwa Ngwaahịa

Akara Ngwaahịa

Nhazi:

ISO 2560-A-E35 0 RA 12

AWS A5.1: E6013

GB/T 5117 E4313

Àgwà:

AWS A5.1 E6013(J421X) bụ elektrọd ụdị rutile. Enwere ike ịgbado ọkụ ma isi iyi ike AC na DC ma ọ nwere ike ịdị maka ọnọdụ niile. Ọ nwere arụmọrụ ịgbado ọkụ dị mma dịka arc kwụsiri ike, obere splatter, iwepụ slag dị mfe na ikike remainition wdg. Rutile-cellulosic electrode nwere ikike ịgbado ọkụ dị mma n'ọnọdụ niile gụnyere ala kwụ ọtọ. Ike ịgbado oghere dị mma na arc-striking. Maka ịgbado ọkụ tack na ntinye ibu. Ebumnuche izugbe maka ụlọ ọrụ na azụmaahịa, mgbakọ na ịgbado ọkụ ụlọ ahịa.

Ngwakọta Kemịkalụnke ígwè Weld niile:(%)
Ngwakọta Kemịkalụ C Mn Si S P Ni Cr Mo V
Ihe achọrọ ≤0.10 0.32-0.55 ≤0.30 ≤0.030 ≤0.035 ≤0.30 ≤0.20 ≤0.30 ≤0.08
Nsonaazụ Ndị A Na-ahụkarị 0.08 0.37 0.18 0.020 0.025 0.030 0.035 0.005 0.004
Njirimara Mechanical nke Metal E tinyere n'ime ya
Ihe Nnwale Rm (N/mm2) Rel (N/mm2) A (%) KV2(J) 0℃
Ihe achọrọ 440-560 ≥355 ≥22 ≥47
Nsonaazụ Ndị A Na-ahụkarị 500 430 27 80
Ugbu a (DC)
Dayameta φ2.0 φ2.5 φ3.2 φ4.0 φ5.0
Ampereji 40 ~ 70 50 ~ 90 80~ 130 150 ~ 210 180 ~ 240

Ọnọdụ ịgbado ọkụ:

PA, PB, PC, PD, PE, PF

Nnyocha redio X-ray:

ỌkwaⅡ

Nlebara anya:

N'ozuzu, mee'Ọ dịghị mkpa ka e jiri electrode ahụ kpọọ nkụ ọzọ tupu ịgbado ọkụ. Ọ bụrụ na mmiri dị n'ime ya emetụta ya, a ga-akpọghachi ya nkụ na 150℃-170℃maka 0.5-1 awa.


  • Nke gara aga:
  • Osote: