Waya Ngwunye Nickel Alloy ERNiCrCoMo-1 Nickel Tig Waya Ihe Njupụta Metal

Nkọwa Dị Mkpirikpi:

Alloy 617 (ERNiCrCoMo-1) bụ waya okpomọkụ dị elu nke ejiri mee ihe maka ịgbado ọkụ nke alloys nickel-chromium-cobalt-molybdenum.


Nkọwa Ngwaahịa

Akara Ngwaahịa

Alloy NickelWaya ịgbado ọkụWaya TigERNiCrCoMo-1

 

Ụkpụrụ
EN ISO 18274 - Ni 6617 - NiCr22Co12Mo9
AWS A5.14 – ER NiCrCoMo-1

 

Atụmatụ na Ngwa

Alloy 617 bụ waya okpomọkụ dị elu nke eji eme ihe maka ịgbado ọkụnikel- ihe ndị e ji chromium-cobalt-molybdenum mee.

Ọ dị mma maka mkpuchi mkpuchi ebe achọrọ ihe yiri ya, dịka turbine gas na ngwa ethylene.

Ọ dabara adaba maka ijikọ alloys dị iche iche ebe a chọrọ ike okpomọkụ dị elu na iguzogide oxidation ruo ihe dị ka 1150°C.

A na-ejikarị ya eme ihe n'ụlọ ọrụ mmepụta ihe dị iche iche dịka na mbara igwe na ike eletrik, dịka petrochemical maka ngwa dịka nitric acid catalyst grids wdg.

Ihe Ndị A Na-ahụkarị Maka Isi

Ngwakọta Inconel 600 na 601, Ngwakọta Incoloy 800 HT na 802 na ngwakọta dịka HK40, HP na HP45 Modified. Nọmba UNS N06617, 2.4663, 1.4952, 1.4958, 1.4959, NiCr21Co12Mo, X6CrNiNbN 25 20, X5NiCrAlTi 31 20, X8NiCrAlTi 32 21, Ngwakọta 617, N08810, N08811*
* Ndepụta ihe atụ, ọ bụghị nke zuru oke

 

 

Ihe mejupụtara kemịkalụ%

C%

Mn%

Fe%

P%

S%

Si%

Cu%

0.05

kachasị

kachasị

kachasị

kachasị

kachasị

kachasị

0.10

1.00

1.00

0.020

0.015

0.50

0.50

Ni%

Kọ%

Al%

Ti%

Cr%

Mo%

44.00

10.00

0.80

kachasị

20.00

8.00

nkeji

14.00

1.50

0.60

24.00

10.00

 

Njirimara Mekaniki
Ike ọdụdọ ≥620 MPa
Ike Mwepụta -
Ogologo -
Ike Mmetụta -

Njirimara igwe dị nso ma nwee ike ịdị iche dabere na okpomọkụ, gas nchekwa, paramita ịgbado ọkụ na ihe ndị ọzọ.

 

Gas Nchedo

TS EN ISO 14175 - TIG: I1 (Argon)

 

Ọnọdụ ịgbado ọkụ

TS EN ISO 6947-PA, PB, PC, PD, PE, PF, PG

 

Data Nkwakọ ngwaahịa

Dayameta

Ogologo

Ibu

1.60 mm

2.40 mm

3.20 mm

1000 mm

1000 mm

1000 mm

5 n'arọ

5 n'arọ

5 n'arọ

 