Nickel Alloy Welding Waya ERNi-1 Nickel Tig Wire Filler Metal

Nkọwa dị mkpirikpi:

A na-eji ER-Ni1 maka ịgbado ọkụ na mkpuchi nke Nickel 200 na Nickel 201 alloys.


Nkọwa ngwaahịa

Mkpado ngwaahịa

Nickel AlloyWaya ịgbado ọkụTig WayaERNi-1

Ụkpụrụ
EN ISO 18274 - Ni 2061 - NiTi3
AWS A5.14 – ER Ni-1

 

Atụmatụ na ngwa

A na-eji ER-Ni1 maka ịgbado ọkụ na mkpuchi nke Nickel 200 na Nickel 201 alloys.

Zuru okè maka ijikọ Monel alloys na ọla kọpa-nickelalloys ka carbon steels.

Ni1 nwere titanium zuru oke iji chịkwaa porosity weld-metal na usoro ịgbado ọkụ.

A na-ejikarị na ụlọ ọrụ nhazi kemịkalụ, mmepụta eriri sịntetik & akụrụngwa nhazi nri wdg.

 

Ngwa ndị isi a na-ahụkarị

Nickel 200 na 201*
* Ihe atụ, ọ bụghị ndepụta zuru oke

 

Ngwakọta kemịkalụ%
C% Mn% Fe% P% S% Si%  
max max max max max max  
0.05 0.80 0.70 0,030 0.010 0.75  
             
Cu% Ni% Co% Ti% Al%    
max 93.00 max 2.00 max    
0.20 min 1.00 3.50 1.00    

 

Ihe eji arụ ọrụ
Ike ọdụdọ ≥410 MPa  
Mpụta Ike ≥200 MPa  
Ogologo oge ≥30%  
Mmetụta Mmetụta ≥100 J  

Ngwongwo eji arụ ọrụ dị ihe dị ka ma nwee ike ịdịgasị iche dabere na ọkụ, ikuku mkpuchi, paramita ịgbado ọkụ na ihe ndị ọzọ.

 

Gases na-echebe

TS EN ISO 14175 - TIG: I1 (Argon)

 

Ọnọdụ ịgbado ọkụ

TS EN ISO 6947-PA, PB, PC, PD, PE, PF, PG

 

Data nkwakọ
Dayameta Ogologo Ibu  
1.60 mm

2.40 mm

1000 mm

1000 mm

5 n'arọ

5 n'arọ

 

 