Onye na-eweta ihe eji agbado ọkụ EM14KS Waya Welding Arc Submerged, Carbon Steel Rod maka ịgbado ọkụ n'ime mmiri Arc.

Nkọwa dị mkpirikpi:

EM14KS bụ eriri igwe, carbon steel electrode maka ịgbado ọkụ n'ime mmiri.


Nkọwa ngwaahịa

Mkpado ngwaahịa

EM14KS bụ eriri igwe, carbon steel electrode maka ịgbado ọkụ n'ime mmiri.Ezubere ya maka ịgbado ọkụ otu na otutu ngafe nke carbon, yana ụfọdụ alloy dị ala, nchara n'ọnọdụ ewepụghị na kehoraizin fillet.Họrọ EM14KS nwere obere mgbakwunye nke titanium nke na-eme ka ike igwe weld dị mma ma na-enyere aka ịnọgide na-enwe ike mgbe ọ kwụsịrị nchekasị.Ekwesịrị iji electrode a maka ịgbado ọkụ n'ime mmiri naanị.

NKWUKWU:

EC1 kwa AWS A5.17, SFA 5.17.

ÀJÀ:

Họrọ EM14KS ka emebere kemịkalụ nkwụnye ego weld dabara na nke waya siri ike mepụta, EM14K electrodes.Nhazi waya cored na-ebute ọnụego nkwụnye ego dị elu karịa waya siri ike mgbe a na-agba ọsọ n'otu ọkwa dị ugbu a.

Họrọ EM14KS na-enye ohere maka njikwa ntinye bead ka mma karịa waya siri ike.Usoro ntinye maka electrode cored ka sara mbara ma na-emighị emi dị ntakịrị, na-ebelata ọchịchọ nke ọkụ site na mgbọrọgwụ mgbọrọgwụ ma ọ bụ na-adabaghị na nkwonkwo.

Ngwa:

Họrọ EM14KS dị mma maka ngwa ndị ahụ metụtara ịgbado ọkụ nke arịa nrụgide na nchara carbon arụ ọrụ dịka A36, A285, A515, na A516.Ekwesịrị iji ya mee ihe na-anọpụ iche ma nwee ike dochie ya ebe ọ bụla waya siri ike, a na-eji EM14K electrode.

CHEMISTERY ONYE NKWUKWU:

Wt%

C

Mn

P

S

Si

Ti

.06

1.55

.015

.015

.55

.05

NDỤMỌDỤ NDỊ NA-AGBADO akwadoro:

5/64”

Amps
250

Volt
26-27

WFS (ipm)
90

ESO (n'ime)
¾"-1¼"

Ọnụọgụ ego (lb / h)
6.5

350

29-30

160

11

500

33-34

290

20

3/32"

275

28-29

80

1"-1¼"

8.5

450

32-33

155

15.5

600

37-38

245

24.7

1/8"

400

28-29

68

1"-1¼"

11.5

550

32-33

100

17

750

37-38

150

26.5

5/32”

425

30-31

45

1¼"-1½"

11.5

650

34-35

80

18.5

900

40-42

140

38