E9015-B3 obere ihe eji agbado ígwè

Nkọwa Dị Mkpirikpi:

Electrodes maka ígwè ndị na-eguzogide creep


Nkọwa Ngwaahịa

Akara Ngwaahịa

AWS: SFA 5.5 E9015-B3Electrodes maka ígwè ndị na-eguzogide creep

E tinyere obere elektrọd hydrogen 2.25Cr – 1Mo nke nwere ike ịgbado ọkụ, na-egosipụta ike dị egwu na iguzogide mmiri na okpomọkụ dị elu ruo 575C. A na-eji ya agbado ọkụ 21/4 Cr-1 Mo nke na-eguzogide mmiri na ígwè Cr-Mo-V nke na-eguzogide mmiri na hydrogen n'okpuru nrụgide yana maka ígwè a kpụrụ akpụ nke nwere ihe mejupụtara yiri nke ígwè ịgbado ọkụ. Ihe ndị a na-ejikarị eme ihe gụnyere owuwu nke steam boiler, ịgbado ọkụ nke steam na ọkpọkọ super-heater, ụlọ ọrụ ike, ụlọ ọrụ mmanụ na ụlọ ọrụ kemịkalụ.

Ihe mejupụtara kemịkalụ nke ígwè niile e ji welded mee (%)

Ihe C Mn Si P S Cr Mo
Pasentị 0.05-0.12 0.5-0.9 ≤0.5 ≤0.030 0.022 2.0-2.5 0.9-1.2

Njirimara MEKANỊKỤ nke Ígwè Weld niile

(PWHT: 690°C maka otu awa)

UTS YS Ogologo
(MPa) (MPa) (L= 4d)%
≥590 550 ≥15

DATA UGBU A NA NKWAKỌTA: DC (+)

Nha (mm)

5×450

4×450

3.15 × 450

2.5 × 350

Oke Ugbu a (Amps)

200-250

150-190

100-140

70-100

Ọnụọgụ (Pcs./Carton)

35

55

75

100

Ịkpachara Anya

1. Kpoo elektrọd ndị ahụ ọzọ na okpomọkụ 250-300 C ruo otu awa, dịka anyị si kwuo.

2. Jiri obere arc na stringer bead mee ihe.


  • Nke gara aga:
  • Osote: