A5.13 ECoCr-C Cobalt Alloy Alloy Hardfacing Welding Rods Yiri Electrode Arc Welding Stick na-eguzogide ọgwụ.

Nkọwa dị mkpirikpi:

A5.13 ECoCr-C Cobalt Alloy Hardfacing Welding Rods na-eji maka ịgbado isi valvụ, akara mgbanaka nke elu nrụgide mgbapụta na akụkụ nke crushers.


Nkọwa ngwaahịa

Mkpado ngwaahịa

 

Nkọwa AWS:AWS A5.13/AME A5.13 ECoCr-C
Ngwa:

Mkpuchi siri ike nke isi valvụ, mgbanaka akara nke mgbapụta nrụgide dị elu na akụkụ nke ndị na-akụpịa ihe.
Nkọwa:

COBALTHARD 1FC kpuchiri electrode bụ alloy ọkọlọtọ siri ike kachasị elu n'ime otu cobalt alloys ejiri maka akwa abrasive okpomọkụ jikọtara ya na corrosion.Nkwụnye ego nke alloy a nwere nnukwu olu nke chromium carbide na-emetụta nguzogide abrasive pụtara ìhè.Mgbakwunye nke tungsten na-eme ka ike ike dị elu na matriks siri ike maka ezigbo nrapado na ihe siri ike na-emebi emebi na-eyi nguzogide.Ọ na-ejikọta nke ọma na nchara niile, gụnyere igwe anaghị agba nchara.
IHE MERE NA OKWU:

Kpoo ọkụ na 300ºC na karịa n'ozuzu.Jiri PHILARC okpomọkụ na-egosi osisi ma ọ bụ PHILARC interpass okpomọkụ nlele iji chọpụta ma a na-enweta okpomọkụ kwesịrị ekwesị tupu ịgbado ọkụ.Maka nkọwa ndị ọzọ hụ PHILARC Chart 4 Nzọụkwụ dị mfe maka ịgbado ọkụ.

Ọ dị irè iji kpoo ọkụ na 600ºC yana iji mee ka ọ dị jụụ mgbe ịgbado ọkụ ga-egbochi mgbawa.

Kpochapụ electrodes na 150-200ºC maka nkeji 30-60 tupu eji ya.Jiri PHILARC obere igwe nkụ nkụ.

Isi ike nke nkwụnye ego ígwè welded: 50 - 56 HRC (520-620 Hv)
NKWUKWU kemịkal nke igwe welded (%):

C Si Mn Cr W Co
2.15 0.47 1.03 31.25 12.72 Bal

Nha dị ugbu a na akwadoro (DC +):

Nha (dia.mm) 3.2 4.0 5.0
Ogologo (mm) 350 350 350
Oke dị ugbu a (Amp) 90-120 110-150 140-180

 

 