AWS: SFA 5.4 E318-16 Igwe anaghị agba nchara Electrodes, mkpanaka ịgbado ọkụ kacha mma

Nkọwa dị mkpirikpi:

A212 (AWS E318-16) bụ obere carbon carbon Cr18Ni12MoNb igwe anaghị agba nchara nwere niobium nwere stabilizer nwere mkpuchi titanium-calcium.


Nkọwa ngwaahịa

Mkpado ngwaahịa

Igwe anaghị agba nchara Electrode

A212

GB/T E318-16

AWS A5.4 E318-16

Nkọwa: A212 bụ obere carbon carbon Cr18Ni12MoNb igwe anaghị agba nchara nwere niobium nwere stabilizer nwere mkpuchi titanium-calcium.Enwere ike iji ya maka ma AC na DC na arụmọrụ arụmọrụ dị mma.Igwe a na-echekwara nwere arụ ọrụ corrosion intergranular dị mma karịa A202 na A207.

Ngwa: Eji maka ịgbado ọkụ dị mkpa 06Cr17Ni12Mo2, ultra-low carbon Cr17Ni14Mo2 na igwe anaghị agba nchara ndị ọzọ, dị ka urea synthesis tower, vinylon akụrụngwa na akụkụ ndị ọzọ kpughere ike corrosive media.

 

 

Ngwakọta kemịkalụ nke igwe weld (%):

C

Mn

Si

Cr

Ni

Nb

Mo

Cu

S

P

≤0.08

0.5-2.5

≤0.90

17.0 ~ 20.0

11.0 ~ 14.0

6 XC ~ 1.00

2.0 ~ 3.0

≤0.75

≤0.030

≤0.040

 

Njirimara nke igwe weld metal:

Nwalee ihe

Ike ọdụdọ

Mpa

Ogologo oge

%

Ekwenyere

≥550

≥25

 

Akwadoro ugbu a:

Dayameta mkpanaka

(mm)

2.0

2.5

3.2

4.0

5.0

Welding Ugbu a

(A)

25 ~ 50

50 ~ 80

80 ~ 110

110 ~ 160

160 ~ 200

 

Mara:

1. The electrode ga-abụọ maka 1 hour na gburugburu 150 ℃ tupu ịgbado ọkụ ọrụ;

2. N'ihi na penetration omimi bụ na-emighị emi n'oge AC ịgbado ọkụ, na DC ike ọkọnọ ga-eji dị ukwuu dị ka o kwere mee ka miri penetration.na nke ugbu a ekwesịghị ịbụ oke buru ibu iji zere ịcha ọbara ọbara nke mkpanaka ịgbado ọkụ;

3. A na-ekpebi nguzogide corrosion nke ọla edobere site na nkwekọrịta abụọ nke ọkọnọ na ọchịchọ.

 

Wenzhou Tianyu Electronic Co., Ltd. e guzobere na 2000. Anyị na-etinye aka na mmepụta nke electrodes ịgbado ọkụ, mkpara ịgbado ọkụ, na ịgbado ọkụ consumables n'ihi na ihe karịrị 20 afọ.

Ngwaahịa anyị bụ isi gụnyere igwe anaghị agba nchara igwe anaghị agba nchara, carbon steel ịgbado ọkụ electrodes, ala alloy ịgbado ọkụ electrodes, surfacing ịgbado ọkụ electrodes, nickel & cobalt alloy ịgbado ọkụ electrodes, nwayọọ ígwè & ala alloy ịgbado ọkụ wires, igwe anaghị agba nchara welding wires, gas-shielded flux cored wires, waya ịgbado ọkụ aluminom, ịgbado ọkụ n'okpuru mmiri.wires, nickel & cobalt alloy welding wires, brass welding wires, TIG & MIG welding wires, tungsten electrodes, carbon gouging electrodes, na ndị ọzọ ịgbado ọkụ ngwa & consumables.

 

 