W707Ni Low Temperate Steel Welding Electrode Low-Hydrogen Stick Welding Suppliers

Nkọwa dị mkpirikpi:

W707Ni bụ igwe nchara dị ala nke nwere Ni na mkpuchi sodium dị ala.


Nkọwa ngwaahịa

Mkpado ngwaahịa

Igwe Okpomọkụ dị alaịgbado ọkụElectrode

W707Ni                                                     

GB/T E5515-C1

Nkọwa: W707Ni bụ electrode ígwè dị ala nke nwere Ni na mkpuchi sodium dị ala.Jiri DCEP (nke dị ugbu a nke ọma) ma nwee ike ịgbanye ya n'ọnọdụ niile.Ọla edobere ka nwere mmetụta siri ike na -70 Celsius.

Ngwa: Ejiri ya maka ịgbado ọkụ dị ala dị ka 2.5Ni.

 

Ngwakọta kemịkalụ nke igwe weld (%):

C

Mn

Si

Ni

S

P

≤0.12

≤1.25

≤0.60

2.00 ~ 2.75

≤0.020

≤0.025

 

Njirimara nke igwe weld metal:

Nwalee ihe

Ike ọdụdọ

Mpa

Mpụta ike

Mpa

Ogologo oge

%

Uru mmetụta (J)

-70 ℃

Ekwenyere

≥540

≥440

≥17

≥27

 

Mgbasa hydrogen ọdịnaya nke ọla edobere: ≤6.0mL/100g (glycerin usoro) ma ọ bụ ≤10mL/100g (mercury ma ọ bụ gas chromatography usoro)

Nyocha x-ray: akara ule

 

Akwadoro ugbu a:

(mm)

Dayameta mkpanaka

2.0

2.5

3.2

4.0

5.0

(A)

Welding Ugbu a

40 ~ 70

60 ~ 90

90 ~ 120

140 ~ 180

170-210

 Mara:

  1. The electrode ga-abụọ maka 1 hour na 350 ℃ tupu ịgbado ọkụ ọrụ;
  2. Ọ dị mkpa iji kpochaa nchara, ọnụ ọgụgụ mmanụ, mmiri, na adịghị ọcha na akụkụ ịgbado ọkụ tupu ịgbado ọkụ;
  3. Gbalịa iji obere ike ahịrị mgbe ị na-agbado, multi-layer na multi-pass welding.

 