RBCuZn-B (Nickel Bronze) Brazing Filler Metals Welding Waya

Nkọwa dị mkpirikpi:

RBCuZn-B Nickel Bronze (RBCuZn-B) brazing metal filler yiri bronze ụgbọ mmiri mana ọ nwere manganese na ígwè nke na-abawanye ike na ike nke nkwụnye ego weld.


Nkọwa ngwaahịa

Mkpado ngwaahịa

RBCuZn-B Nickel Bronze (RBCuZn-B) brazing metal filler yiri bronze ụgbọ mmiri mana ọ nwere manganese na ígwè nke na-abawanye ike na ike nke nkwụnye ego weld.O nwekwara nickel na-ahụ maka nkesa otu ígwè na nkwụnye ego ahụ.Ekwesịrị iji ọkụ na-anọpụ iche ma ọ bụ ntakịrị oxidizing na ụdị boric acid/boric flux.

Klas AWS: RBCuZn-B Asambodo: AWS A5.8/A5.8M:2011
Alloy: RBCuZn-B ASME SFA A5.8

 

Ọnọdụ mgbụsị akwụkwọ: H, V Oke mgbawa:
1620-1800F

 

Ike tensile, kpsi: 60-78
Nkwalite%, nkeji: 25

 

Ebe Na-agbaze 1620F Nkwado 1590F Brinell Hardness 80-110

Chemistry Waya a na-ahụkarị dị ka AWS A5.8 (ụkpụrụ otu kacha)

Cu Zn Sn Fe Mn Ni Pb Al Si Ndị ọzọ
56.0-60.0 Rem 0.80-1.10 0.25-1.20 0.01-0.50 0.20-0.80 0.05 0.01 0.04-0.20 0,50

 

Wenzhou Tianyu Electronic Co., Ltd. e guzobere na 2000. Anyị na-etinye aka na mmepụta nke electrodes ịgbado ọkụ, mkpara ịgbado ọkụ, na ịgbado ọkụ consumables n'ihi na ihe karịrị 20 afọ.

Ngwaahịa anyị bụ isi gụnyere igwe anaghị agba nchara igwe anaghị agba nchara, carbon steel ịgbado ọkụ electrodes, ala alloy ịgbado ọkụ electrodes, surfacing ịgbado ọkụ electrodes, nickel & cobalt alloy ịgbado ọkụ electrodes, nwayọọ ígwè & ala alloy ịgbado ọkụ wires, igwe anaghị agba nchara welding wires, gas-shielded flux cored wires, waya ịgbado ọkụ aluminom, ịgbado ọkụ n'okpuru mmiri.wires, nickel & cobalt alloy welding wires, brass welding wires, TIG & MIG welding wires, tungsten electrodes, carbon gouging electrodes, na ndị ọzọ ịgbado ọkụ ngwa & consumables.

 

 

 

 