Waya Ngwugwu Alloy Nickel Alloy ERNiCrMo-3 Tig Waya

Nkọwa Dị Mkpirikpi:

ERNiCrMo-3 bụ waya alloy nickel dị elu nke e mepụtara maka ịgbado ọkụ na mkpuchi alloy dabere na nickel dịka 625 ma ọ bụ ihe yiri ya.


Nkọwa Ngwaahịa

Akara Ngwaahịa

Alloy NickelWaya ịgbado ọkụWaya TigERNiCrMo-3

 

Atụmatụ na Ngwa

Elunikelwaya alloy emepụtara maka ịgbado ọkụ na mkpuchinikel-a na-eji ihe ndị yiri ya eme ihe dịka 625 ma ọ bụ ihe yiri ya.

E sere ya nke ọma n'ụzọ pụrụ iche iji nweta njikọta dị ọcha ma dị elu nke nwere akwa na-egbuke egbuke na ezigbo ductility.

Ọkụ ígwè ahụ nwere ezigbo ihe eji arụ ọrụ n'ime ya n'oge okpomọkụ dị elu na nke dị ala.

Nguzogide dị mma megide nsị na nrụgide nke mmebi.

Okpomọkụ ọrụ akwadoro sitere na cryogenic ruo 540°C.

A na-ejikarị ya eme ihe n'ụlọ ọrụ mmepụta kemịkalụ, injinịa mmiri, ihe ndị na-eme ka ihe dị n'ime nuklia, ụgbọelu na akụrụngwa njikwa mmetọ wdg.

Ihe Ndị A Na-ahụkarị Maka Isi

Inconel 601, Incoloy 800, Alloy 625, Alloy 825, Alloy 926*
* Ndepụta ihe atụ, ọ bụghị nke zuru oke

 

Ụkpụrụ
TS EN ISO 18274 - Ni 6625 - NiCr22Mo9Nb
AWS A5.14 – ER NiCrMo-3

 

Ihe mejupụtara kemịkalụ%

C%

Mn%

Fe%

P%

S%

Si%

Cu%

kachasị

kachasị

kachasị

kachasị

kachasị

kachasị

kachasị

0.10

0.50

0.50

0.015

0.015

0.50

0.50

Ni%

Kọ%

Al%

Ti%

Cr%

Nb+Ta%

Mo%

60.00

kachasị

kachasị

kachasị

20.00

3.15

8.00

nkeji

1.0

0.40

0.40

23.00

4.15

10.00

 

Njirimara Mekaniki
Ike ọdụdọ ≥760 MPa  
Ike Mwepụta ≥415 MPa  
Ogologo ≥35%  
Ike Mmetụta ≥100 J  

Njirimara igwe dị nso ma nwee ike ịdị iche dabere na okpomọkụ, gas nchekwa, paramita ịgbado ọkụ na ihe ndị ọzọ.

 

Gas Nchedo

TS EN ISO 14175 - TIG: I1 (Argon)

 

Ọnọdụ ịgbado ọkụ

TS EN ISO 6947-PA, PB, PC, PD, PE, PF, PG

 

Data Nkwakọ ngwaahịa
Dayameta Ogologo Ibu  
1.60 mm

2.40 mm

3.20 mm

1000 mm

1000 mm

1000 mm

5 n'arọ

5 n'arọ

5 n'arọ

 

 

Ibu Ọrụ: Ọ bụ ezie na emeela mgbalị niile ezi uche dị na ya iji hụ na ozi dị na ya ziri ezi, ozi a nwere ike ịgbanwe na-enweghị ọkwa ma enwere ike iwere ya dị ka nke dabara adaba maka nduzi izugbe.

 


  • Nke gara aga:
  • Osote: