Ngwugwu Ni327-6 nke Nikel Alloy nke na-agbakọta ọnụ AWS A5.11 ENiCrMo-6 nke na-agbakọta ọnụ, ...

Nkọwa Dị Mkpirikpi:

Ni327 -6 (AWS A5.11 ENiCrMo-6) bụ elektrọd dabere na nickel nwere mkpuchi sodium dị ala. Jiri DCEP (elektrọd positive ozugbo).


Nkọwa Ngwaahịa

Akara Ngwaahịa

Ngwunye Electrode nke Nickel na Nickel Alloy

Ni327-6                                                     

GB/T ENi6620

AWS A5.11 ENiCrMo-6

Nkọwa: Ni327 -6 bụ elektrọd dabere na nickel nwere mkpuchi sodium dị ala. Jiri DCEP (elektrọd ugbu a kpọmkwem).dị mma). Ígwè e tinyere n'ime ya nwere ezigbo ike, ike na nguzogide mgbawa. Ígwè e tinyere n'ime ya nwere oke mgbasawanye yiri nke ígwè, ma nwee ike dị elu na nguzogide siri ike na nguzogide nchara n'oge okpomọkụ ụlọ na okpomọkụ dị elu.

Ngwa: A na-eji ya agbakọta ígwè Ni9%, a pụkwara iji ya agbakọta ígwè dị iche iche na alloys siri ike ịgbado ọkụ.

 

Ngwakọta kemịkalụ nke ígwè weld(%):

C

Mn

Si

Ni

Mo

Fe

Cu

≤0.10

2.0 ~ 4.0

≤1.0

≥55.0

5.0 ~ 9.0

≤10.0

≤0.5

Nb + Ta

W

Cr

S

P

Ndị ọzọ

 

0.5 ~ 2.0

1.0 ~ 2.0

12.0 ~ 17.0

≤0.015

≤0.020

≤0.5

 

 

Njirimara mekaniki nke igwe weld:

Ihe nnwale

Ike ọdụdọ

Mpa

Ike mmeputa

Mpa

Ogologo

%

Ekwere nkwa

≥620

≥350

≥32

 

Ugbu a akwadoro:

Dayameta mkpanaka

(mm)

2.5

3.2

4.0

Ịgbado ọkụ ugbu a

(A)

50 ~ 70

80 ~ 100

110 ~ 150

 

Rịba ama:

1. A ga-emerịrị elektrọd ahụ ruo otu awa na ihe dị ka 300℃ tupu a rụọ ọrụ ịgbado ọkụ. Gbalịa iji obere arc iji gbado ọkụ;

2. Ọ dị mkpa ịsacha ihe ndị ruru unyi, mmanụ, mmiri, na ihe ndị na-adịghị mma dị n'akụkụ ịgbado ọkụ tupu ịgbado ọkụ.

3. Gbalịa iji obere ike ahịrị mgbe ị na-agbado ọkụ, ịgbado ọkụ ọtụtụ oyi akwa na ịgbado ọkụ ọtụtụ ngafe.

 

 


  • Nke gara aga:
  • Osote: