Nkọwa Dị Mkpirikpi:

DIN 8555 (E9-UM-250-KR) bụ elektrọd pụrụ iche nwere ezigbo njikọta na ihe eji arụ ọrụ. Austenite - Ferrites na-eji ígwè agbakọta. Ike dị elu na oke ike mgbawa.


Nkọwa Ngwaahịa

Akara Ngwaahịa

Ịgbado ọkụ siri ikeElektrọd

Ọkọlọtọ: DIN 8555 (E9-UM-250-KR)

Ụdị Nọmba: TY-C65

 

Nkọwapụta na Ngwa:   

· Elektrọd pụrụ iche nwere ezigbo ihe eji agbado ọkụ na ihe eji arụ ọrụ.

· Austenite - Ferrites na-eji ígwè agbakọta. Uru dị elu na ike dị elu na ike mgbawa dị elu.

· Ọ kacha mma maka ijikọ na ígwè ndị na-anaghị agbakọta agbakọta, mgbe a na-achọkarị ihe kachasị mkpa na njikọta ahụ.

· Nguzogide mgbawa dị elu mgbe ejikọtara ígwè ndị nwere ike ịgbado ọkụ siri ike, dịka ígwè austenitic na ferritic, ígwè nwere nnukwu manganese nwere ígwè ndị a gwakọtara agwakọta na ndị na-abụghị nke a gwakọtara agwakọta, ígwè ndị a na-agwọ ọkụ na ngwaọrụ. Ngwa na nrụzi na nrụzi nke akụkụ igwe na draịva yana n'ịrụzi ngwaọrụ.

· Dịka ihe mkpuchi isi dị n'elu ihe ndị a dịkwa mma nke ọma.

 

 

Ngwakọta kemịkalụ nke ígwè e tinyere n'ime ya(%):

 

C

Si

Mn

P

S

Cr

Ni

Mo

N

Fe

DIN

-

0.15

-

0.90

0.50

2.50

-

0.04

-

0.03

28.0

32.0

8.0

10.0

-

-

Bọl.

Nkịtị nkịtị

0.1

1.0

1.0

≤0.035

≤0.025

29.0

9.0

≤0.75

0.10

Bọl.

 

Ike nke ígwè e tinyere n'ime ya:

Ike mmeputa

Mpa

Ike ọdụdọ

Mpa

Ogologo

A(%)

Ike Dị ka welded

(HB)

620

narị asatọ

22

240

 

Àgwà Izugbe:

· Sistemụ obere Austenite + Ferrite

· Ịrụ ọrụ dị mma nke ukwuu

· Kpoo ọkụ tupu oge eruo Ịkpo ọkụ tupu oge eruo nke akụkụ ferritic dị arọ ruo 150-150℃

· Ịchacha Redry ruo awa 2 na okpomọkụ 150-200℃ tupu e jiri ya.

 

 