D237 (B-84) Electrode ịgbado ọkụ siri ike, mkpanaka ịgbado ọkụ dị n'elu, mkpịrị ịgbado ọkụ

Nkọwa dị mkpirikpi:

D237 (B-84) bụ electrode maka mkpuchi siri ike na alloy steels na carbon steels.The beads na elu dị larịị, nke na-enweghị mgbawa na pores, na-etinye ihe siri ike nke na-eguzogide ọgwụ mgbochi na mmetụta nke ọkara.Ọ dị mfe ịgbado ọkụ n'ọkwa niile ma ewezuga vetikal ala.


Nkọwa ngwaahịa

Mkpado ngwaahịa

Mgbado ọkụ ọkụ ọkụ ElectrodeRODO P

ARA RECUBRIMIENTO PROTECTOR

Ụdị Nọmba: D237 (B-84) 

Nyocha igwe etinyere ego (Ụkpụrụ ahụkarị)

C

Mn

Si

Cr

Mo

V

0.5%

0.3%

0.7%

7%

0.5%

0.5%

 

Njirimara:

B- 84 bụ electrode maka mkpuchi siri ike na alloy steels na carbon steel.The beads na elu dị larịị, nke na-enweghị mgbawa na pores, na-etinye ihe siri ike nke na-eguzogide ọgwụ mgbochi na mmetụta nke ọkara.Ọ dị mfe ịgbado ọkụ n'ọkwa niile ma ewezuga vetikal ala.

Ngwongwo igwe:Isi ike sitere na 55 ruo 60 HRc (nke oyi akwa)

Ọkwa ịgbado ọkụ:Flat, kwụ ọtọ, elu, kwụ ọtọ elu.

 

Ugbu a na Polarity:

Maka mgbanwe ma ọ bụ ozugbo

Electrode na ogwe osisi dị mma

nke mm

ø in

Amperage

3.20

1/8

100-130

4.00

5/32

120-160

5.00

2/16

180-220

 

Ngwa: • Ọ dị mma maka ịmegharị akụrụngwa ebe a na-egwupụta ihe, ikpokọta, igwu mmiri

• Laminating na-apụta

• Igwe igwe na-akpụ akpụ

• Igwe maka mmegharị ụwa

• Akpụkpọ anụ.

 

Ogologo: 350mm.

Arọ kwa igbe: 20 n'arọ/44 lbs.

 

Wenzhou Tianyu Electronic Co., Ltd. e guzobere na 2000. Anyị na-etinye aka na n'ichepụta nkewelding electrodes, mkpanaka ịgbado ọkụ, na welding consumables ihe karịrị afọ 20.

Ngwaahịa anyị bụ isi gụnyere igwe anaghị agba nchara igwe anaghị agba nchara, carbon steel ịgbado ọkụ electrodes, ala alloy ịgbado ọkụ electrodes, surfacing ịgbado ọkụ electrodes, nickel & cobalt alloy ịgbado ọkụ electrodes, nwayọọ ígwè & ala alloy ịgbado ọkụ wires, igwe anaghị agba nchara welding wires, gas-shielded flux cored wires, waya ịgbado ọkụ aluminom, ịgbado ọkụ n'okpuru mmiri.wires, nickel & cobalt alloy welding wires, brass welding wires, TIG & MIG welding wires, tungsten electrodes, carbon gouging electrodes, na ndị ọzọ ịgbado ọkụ ngwa & consumables.

 

 

 

 


  • Nke gara aga:
  • Osote: