H10MnSi AWS EM13K Waya Welding Arc gbara mmiri

Nkọwa dị mkpirikpi:

H10MnSi Submerged arc ịgbado ọkụ waya bụ ụdị nke ọkara-manganese na ọkara-silicon ụdị ịgbado ọkụ waya.


Nkọwa ngwaahịa

Mkpado ngwaahịa

H10MnSi AWS EM13K Waya Welding Arc gbara mmiri

EM13K 2.5/3.2/4.0/5.0mm Waya Welding Arc Submerged

H10MnSi Submerged arc ịgbado ọkụ waya bụ ụdị nke ọkara-manganese na ọkara-silicon ụdị ịgbado ọkụ waya.
1. Ọ dakọtara na ọkara-manganese na ọkara-silicon ụdị ịgbado ọkụ flux.
2. Ọ naghị emetụ nchara na nchara nchara.
3. Ọ nwere ọmarịcha bead ịkpụzi na slag detachability.
4. Monopole ma ọ bụ dipole.AC/DC.
5. A na-eji ya maka ịgbado ọkụ dị elu na ịgbado ọkụ na 50kg klas isi ọla.
6. ịgbado ọkụ nke ọzọ 501 Mpa larịị carbon ígwè na ala alloy ígwè

EM13K kwekọọ na ọkọlọtọ :GB/T 5293 H10MnSi
AWS EM13K
ISO 14171-B-SU25

Nkọwapụta: Ọ bụ ụdị waya ịgbado ọkụ nke nwere manganese na ọdịnaya silicon kwesịrị ekwesị., Ọ dabara na obere manganese na obere silicon ụdị ịgbado ọkụ, enweghị mmetụta na nchara na metal.Ọ nwere ezigbo ịkpụzi bead, ikike ịwepụ slag mara mma.

Nzube: Iji na sintered flux LT.SJ101, ọ nwere ike tinye ma maka elu-ọsọ ịgbado ọkụ ígwè efere nke tensile ike 420N/mm2 na ndochi ịgbado ọkụ.A na-ejikarị ya eme ihe maka ịgbado ọkụ ọkụ, ụgbọ mmiri, akwa mmiri, ụgbọ mmiri wdg.

Ngwakọta kemịkalụ(%)

 

 

Ngwakọta kemịkalụ C Mn Si S P Cr Ni Cu
Uru ekwe nkwa ≤0.14 0,80 ~
1.10
0,60 ~
0.90
≤0.035 ≤0.035 ≤0.20 ≤0.30 ≤0.35
Nsonaazụ izugbe 0.089 0.98 0.67 0.023 0.032 0.015 0.034 0.11

 
Njirimara Mechanical nke ọla edobere

Nwalee ihe

Flux

Rm(MPa) ReL/Rp0.2(MPa) A(%) KV2(J)
-20 ℃
LT•SJ101 415-550 ≥330 ≥22 ≥27

 
Ogo nke Welding Wires

Nha (mm) Φ2.5 Φ3.2 Φ4.0 Φ5.0

 


  • Nke gara aga:
  • Osote: