Mkpanaka ịgbado ígwè ER70S-3 nke e ji ígwè carbon mee, ihe e ji emeju ihe maka waya ịgbado ọkụ, waya Tig na Mig nke e ji gas kpuchie.

Nkọwa Dị Mkpirikpi:

ER70S3 bụ waya MIG maka ọtụtụ ngwa ịgbado ọkụ carbon ígwè.


Nkọwa Ngwaahịa

Akara Ngwaahịa

ER70S-3 Ihe e ji eme ka ígwè jupụta n'ọkụ carbon maka ịgbado ọkụ gas

ER70S3 bụ waya MIG a na-ejikarị eme ihe maka ọtụtụ ngwa ịgbado ígwè carbon. Ọ bụ waya e ji silicon na manganese deoxidized mee ka ọ dị mma maka imepụta ihe n'ozuzu. Ngwaahịa a chọrọ gas na-echebe ya.

Ngwa ndị a na-ejikarị eme ihe: imepụta ihe n'ozuzu, arịa ụlọ ígwè, mpempe akwụkwọ ígwè, imepụta ígwè ịchọ mma, akụrụngwa ugbo

Klas AWS: ER70S3 Asambodo: AWS A5.18/A5.18M:2005
Alloy: ER70S3 ASME SFA A5.18

 

Ọnọdụ ịgbado ọkụ: F, V, OH, H Ugbu a:
MIG-DCEP
TIG-DCEN

 

Ike nrụgide, kpsi: 70
Ike Mmepụta, kpsi: 58
Ogologo na 2"%: 22

Kemịstrị Waya nkịtị dịka AWS A5.18 si dị (otu uru kachasị)

C Mn Si P S Ni Cr Mo V Cu
0.06-0.15 0.90-1.40 0.45-0.75 0.025 0.035 0.15 0.15 0.15 0.03 0.50
Nkịtị ịgbado ọkụ
Dayameta Usoro Volt Amps Gas Nchedo
in (mm)
.035 (0.9) GMAW 28-32 165-200 Nnyefe Fesa 98% Argon+2% Oxygen ma ọ bụ 75% Argon+25% CO2
.045 (1.2) GMAW Afọ 30-34 180-220 Nnyefe Fesa 98% Argon+2% Oxygen ma ọ bụ 75% Argon+25% CO2
1/16 (1.6) GMAW Afọ 30-34 230-260 Nnyefe Fesa 98% Argon+2% Oxygen ma ọ bụ 75% Argon+25% CO2
.035 (0.9) GMAW 22-25 100-140 Nnyefe Njem Obere 100% CO2 ma ọ bụ 75% Argon + 25% CO2
.045 (1.2) GMAW 23-26 120-150 Nnyefe obere sekit 100% CO2 ma ọ bụ 75% Argon + 25% CO
1/16 (1.6) GMAW 23-26 160-200 Nnyefe obere sekit 100% CO2 ma ọ bụ 75% Argon + 25% CO
1/16 (1.6) GTAW 12-15 100-125 Argọn 100%
3/32 (2.4) GTAW 15-20 125-175 Argọn 100%
1/8 (3.2) GTAW 15-20 175-250 Argọn 100%

 