Nkọwa dị mkpirikpi:

ER5356 bụ ụdị aluminom Alloy a na-ejikarị eme ihe bụ nke a na-ahọrọ maka ike ya dị elu.


Nkọwa ngwaahịa

Mkpado ngwaahịa

ER5356 bụ ụdị aluminom Alloy a na-ejikarị eme ihe bụ nke a na-ahọrọ maka ike ya dị elu.Tụkwasị na nke ahụ, ọ na-enyekwa ezigbo nkwụsị nke corrosion mgbe ọ na-ekpuchi mmiri nnu.Ekwesịrị ịtụle ER5356 maka ịgbado ọkụ 5000 usoro aluminum isi ọla.

Ngwa a na-ahụkarị: waya ihe eji agbado ọkụ

Klas AWS: ER5356 Asambodo: AWS A5.10/A5.10M:1999
Alloy: ER5356 AWS/ASME SFA A5.10
Ọnọdụ ịgbado ọkụ:
F, V, OH, H
Ugbu a:
DCEP-GMAW
AC-GTAW
Njirimara ahụkarị (dị ka agbadoro)
Omume: 29% IACS (-0)/27% IACS (-H18)
Ike tensile, kpsi: 38
Agba: Ọcha
Ebe Na-agbaze 1175F Nkwado 1060F Njupụta 0.096 lbs/cu In.
Chemistry Waya a na-ahụkarị dịka AWS A5.10 (ụkpụrụ otu kacha)
Si Fe Cu Mn Mg Cr Zn Ti Ndị ọzọ AL
0.25 0.40 0.10 0.50-1.0 4.7-5.5 0.05-0.20 0.25 0.05-0.20 0.15 Ihe fọdụrụ
Ụdị ịgbado ọkụ a na-ahụkarị
Dayameta Usoro Volt Amps GAS
in (mm)
.030 (.8) GMAW 15-24 60-175 Argon (cfh)
.035 (.9) GMAW 15-27 70-185 Argon (cfh)
3/64” (1.2) GMAW 20-29 125-260 Argon (cfh)
1/16” (1.6) GMAW 24-30 170-300 Argon (cfh)
3/32" (2.4) GMAW 26-31 275-400 Argon (cfh)
Dayameta Usoro Volt Amps GAS
in (mm)
1/16” (1.6) GTAW 15 60-80 Argon (cfh)
3/32" (2.4) GTAW 15 125-160 Argon (cfh)
1/8" (3.2) GTAW 15 190-220 Argon (cfh)
5/32” (4.0) GTAW 15 200-300 Argon (cfh)
3/16” (4.8) GTAW 15-20 330-380 Argon (cfh)

Wenzhou Tianyu Electronic Co., Ltd. e guzobere na 2000. Anyị na-etinye aka na mmepụta nke electrodes ịgbado ọkụ, mkpara ịgbado ọkụ, na ịgbado ọkụ consumables n'ihi na ihe karịrị 20 afọ.

Ngwaahịa anyị bụ isi gụnyere igwe anaghị agba nchara igwe anaghị agba nchara, carbon steel ịgbado ọkụ electrodes, ala alloy ịgbado ọkụ electrodes, surfacing ịgbado ọkụ electrodes, nickel & cobalt alloy ịgbado ọkụ electrodes, nwayọọ ígwè & ala alloy ịgbado ọkụ wires, igwe anaghị agba nchara welding wires, gas-shielded flux cored wires, waya ịgbado ọkụ aluminom, ịgbado ọkụ n'okpuru mmiri.wires, nickel & cobalt alloy welding wires, brass welding wires, TIG & MIG welding wires, tungsten electrodes, carbon gouging electrodes, na ndị ọzọ ịgbado ọkụ ngwa & consumables.

 

 


  • Nke gara aga:
  • Osote: