Mkpanaka na Electrodes ER1100 A5.10 Aluminom Wedding Waya Mig

Nkọwa Dị Mkpirikpi:

ER1100 na-eguzogide ọgwụ ike na nsogbu ikuku. Ọ bụ ihe na-adịghị agbanwe agbanwe nke na-eme ka ọ dị nro ma na-arụkwa ọrụ nke ọma na ngwaahịa gauge na foil dị gịrịgịrị.


Nkọwa Ngwaahịa

Akara Ngwaahịa

ER1100 A5.10, Electrodes na Mkpanaka Aluminom na Aluminom Alloy

ER1100 na-eguzogide ọgwụ ike na nsogbu ihu igwe. Ọ bụ ihe na-adịghị agbanwe agbanwe nke na-eme ka ọ dị nro nke ukwuu, a na-ejikwa ya eme ihe nke ọma na ngwaahịa dị gịrịgịrị na foil. Ọ nwere ezigbo ihe eji eme ka mmiri dị mmiri mmiri, a na-ejikwa ya eme ihe dị ka ihe na-eme ka ihe dị mma maka ịgbado ọkụ. Ihe a na-achọsi ike na ihe na-eme ka ihe dị na ya dị mma bụ ihe na-egbuke egbuke nke a na-enweta site na anodizing.

Ngwa ndị a na-ejikarị eme ihe: mgbanwe okpomọkụ; akụrụngwa njikwa nri; rivets; waya taị; ịgba ígwè

Klas AWS: ER1100 Asambodo: AWS A5.10/ A5.10M:1999
Alloy: ER1100 AWS/ASME SFA A5.10

 

Ọnọdụ ịgbado ọkụ:
F, V, OH, H
Ugbu a:
DCEP-GMAW
AC-GTAW

 

Njirimara nkịtị (dịka welded)

Nhazi: 59% IACS (-12)
Ike nrụgide, kpsi: 13
Agba: Isi awọ
Ebe Mgbaze 1215⁰F Nkwụsi ike 1090⁰F Njupụta 0.098 lbs/cu In.

Kemịstrị Waya nkịtị dịka AWS A5.10 si dị (otu uru kachasị bụ oke)

Si + Fe Cu Mn Zn Ndị ọzọ Al  
0.95 0.05-0.20 0.05 0.10 0.15 Nkeji 99.0  
Nkịtị ịgbado ọkụ
Dayameta Usoro Volt Amps GAS
in (mm)
.030 (.8) GMAW 15-24 60-175 Argọn (cfh)
.035 (.9) GMAW 15-27 70-185 Argọn (cfh)
3/64” (1.2) GMAW 20-29 125-260 Argọn (cfh)
1/16” (1.6) GMAW 24-30 170-300 Argọn (cfh)
3/32” (2.4) GMAW 26-31 275-400 Argọn (cfh)
Dayameta Usoro Volt Amps GAS
in (mm)
1/16” (1.6) GTAW 15 60-80 Argọn (cfh)
3/32” (2.4) GTAW 15 125-160 Argọn (cfh)
1/8” (3.2) GTAW 15 190-220 Argọn (cfh)
5/32” (4.0) GTAW 15 200-300 Argọn (cfh)
3/16” (4.8) GTAW 15-20 330-380 Argọn (cfh)

E guzobere Wenzhou Tianyu Electronic Co., Ltd. n'afọ 2000. Anyị anọwo na-emepụta elektrọd ịgbado ọkụ, mkpanaka ịgbado ọkụ, na ihe oriri ịgbado ọkụ ruo ihe karịrị afọ 20.

Ngwaahịa anyị bụ isi gụnyere elektrọd ịgbado ígwè anaghị agba nchara, elektrọd ịgbado ígwè carbon, elektrọd ịgbado ígwè dị ala, elektrọd ịgbado ọkụ n'elu, elektrọd ịgbado ígwè nickel & cobalt, waya ịgbado ígwè dị nro na nke dị ala, waya ịgbado ígwè anaghị agba nchara, waya ndị nwere ihe mkpuchi gas, waya ịgbado ígwè aluminom, waya ịgbado arc mmiri, waya ịgbado ígwè nickel & cobalt, waya ịgbado ígwè brass, waya ịgbado ígwè TIG & MIG, elektrọd tungsten, elektrọd ịgbado ígwè, na ngwa ịgbado ígwè ndị ọzọ na ihe oriri.

 

 


  • Nke gara aga:
  • Osote: