Mkpanaka ịgbado ọkụ ECoCr-B Cobalt Alloy 12 siri ike nke na-eguzogide iyi, mkpara ịgbado ọkụ Electrode Arc nke na-eguzogide iyi.

Nkọwa Dị Mkpirikpi:

Ụdị Alloy: A5.13, ÍGWÈ SILIRI ELEKỌDỤ NA MKPỌMKPỌRỌ ỊGBỌ ỌKỤ, A5.13


Nkọwa Ngwaahịa

Akara Ngwaahịa

ECoCr-B (Cobalt 12) Electrọde ịgbado ọkụ na-eguzogide iyi nke Cobalt

Ụdị Alloy: A5.13, ÍGWÈ SILIRI ELEKỌDỤ NA MKPỌMKPỌRỌ ỊGBỌ ỌKỤ, A5.13
A pụrụ iwere ECoCr-B Cobalt Alloy 12 dị ka ihe mgbakwunye dị n'etiti Cobalt Alloy 6 na Cobalt Alloy 1. O nwere akụkụ dị elu nke carbide siri ike ma sie ike karịa Cobalt Alloy 6, ọ na-emekwa ka iguzogide mbuze dị ala, mmịpụta, na mmịpụta siri ike dịkwuo elu ebe ọ na-ejigide mmetụta kwesịrị ekwesị na mgbochi cavitation. A na-ejikarị Cobalt Alloy 12 eme ihe n'onwe ya ma ọ bụ na-agba ọsọ megide Cobalt Alloy 6 ma ọ bụ 1. Ọdịnaya tungsten dị elu na-enye ihe onwunwe okpomọkụ ka mma ma e jiri ya tụnyere Cobalt Alloy 6, enwere ike iji ya na okpomọkụ ruo ihe dị ka 700⁰C. A na-ejikarị Cobalt Alloy 12 eme ihe maka ngwaọrụ ịkpụ ihe ndị chọrọ iguzogide mmịpụta, okpomọkụ na mmịpụta.

Ngwa ndị a na-ejikarị eme ihe: ogwe osisi a na-eji yinye akwọ; ezé a na-eji akwọ akwọ; ihe ndị na-egbu egbu a na-eji ekpuchi ihe

Klas AWS: ECoCr-B Asambodo: AWS A5.13/A5.13M:2010
Alloy: ECoCr-B ASME SFA A5.13

 

Ọnọdụ ịgbado ọkụ:
F, V, OH, H
Ugbu a:
*NS

 

Ike nrụgide, kpsi: *NS
Ike Mmepụta, kpsi: *NS
Ogologo pasentị: *NS

* NS Akọwapụtaghị

Kemịstrị Waya nkịtị dịka AWS A5.13 si dị (otu uru kachasị)

C Mn Si Cr Ni Mo Fe W Co Ndị ọzọ
1.0-1.7 2.0 2.0 25-32 3.0 1.0 5.0 7.0-9.5 Rem 1.0

 