E308-16 igwe anaghị agba nchara ịgbado ọkụ elektrọd E308-16

Nkọwa Dị Mkpirikpi:

Electrọde ịgbado ọkụ igwe anaghị agba ncharaE308-16 bụ eriri eletriki nke ụdị titanium maka ígwè anaghị agba nchara carbon dị ala.


  • :
  • Nkọwa Ngwaahịa

    Akara Ngwaahịa

    AWS: SFA 5.4 E308-16 Electrọde ịgbado ọkụ igwe anaghị agba nchara

    E308-16 bụ ụdị titanium ahịrịelektrọd ịgbado ọkụmaka ígwè anaghị agba nchara carbon dị ala karịa.

    Nhazi:

    AWS A5.4 / ASME SFA5.4 E308-16

    JIS Z3221 D308-16

    Nkọwa:

    Electrode ịgbado ọkụ igwe anaghị agba nchara E308-16 bụ ụdị titanium ahịrịelektrọd ịgbado ọkụmaka ígwè anaghị agba nchara carbon dị ala karịa. Ígwè a na-eji agba ígwè nwere ezigbo ihe eji arụ ọrụ ma na-egosi ezigbo iguzogide ire ere dị n'etiti granular n'ihi na ihe dị na carbon dị na ya bụ ≤. 0.04% b. Enwere ike iji ya maka ịgbado ọkụ n'ọnọdụ niile yana arụmọrụ dị mma: arc kwụsiri ike, obere sptters, ọdịdị dị mma nke ịgbado ọkụ. Electrode ịgbado ọkụ na-egosikwa ezigbo àgwà iguzogide okpomọkụ, ọ dịghị mfe ịgbanwe uhie na a naghị emepụta porosity gas.

    Ngwa:

    Ịgbado ígwè nke 18% Cr-8% Ni.

    Ọ dabara adaba maka usoro ịgbado ọkụ nke ejiri obere carbon 022Cr-19Ni10 igwe anaghị agba nchara rụọ, dịka eriri sịntetik, fatịlaịza,

    Ngwa petrochemical, wdg.

     

    Ngwakọta Kemịkalụ nke E tinyere n'ime ígwè (E308L-16) (%)

    ihe C Mn Si Cr Ni S P Cu Mo
    uru ọkọlọtọ ≤0.08 0.5-2.5 ≤0.90 18.0-21.0 9.0-11.0 ≤0.030 ≤0.040 ≤0.75 ≤0.75
    Uru ihe atụ 0.043 1.10 0.78 19.52 9.76 0.012 0.031 0.02 0.032

    Njirimara Mekaniki nke Metal E tinyere n'ime ya (%)

    A ga-ekpebi arụmọrụ mgbochi-corrosion na nhazi ferrite n'etiti onye zụrụ na onye na-ere ahịa.

    ihe Ike nrụgide (MPa) Ogologo (%)
    uru ọkọlọtọ ≥550 ≥25
    Uru ihe atụ 601 41

    Ngwa

    A na-eji ya agbakọta otu ụdị ígwè anaghị agba nchara nke na-eguzogide okpomọkụ, nke na-arụ ọrụ n'okpomọkụ dị elu, a pụkwara iji ya gbaa ígwè chrome buru ibu (dịka Cr15Mo, Cr9Mo, Cr13, Cr28) na ígwè dị iche iche.

    Dayameta (mm)

    2.0

    2.5

    3.2

    4.0

    5.0

    Ọsọ ịgbado ọkụ (A)

    25-50

    Afọ 50-80

    80-110

    110-160

    160-200

    Ugbu a: AC ma ọ bụ DC+

    Ihe edeturu gbasara ojiji:

    1. Debe akàrà ahụ dị mkpụmkpụ dịka o kwere mee.

    2. Wepụ unyi dịka mmanụ na uzuzu n'ime oghere ahụ.

    3. Kpoo elektrọd ndị ahụ na 350 (662) ruo nkeji iri isii tupu e jiri ya

     


  • Nke gara aga:
  • Osote: