AWS ER5183 Aluminom Welding Waya Aluminom MIG Welding Mkpara na Tig Waya

Nkọwa Dị Mkpirikpi:

ER5183 dabara adaba maka ịgbado ọkụ MIG nke aluminom magnesium alloy nke na achọrọ ike nrụgide dị elu, ọ bụrụkwa na ígwè ntọala bụ 5083 ma ọ bụ 5654, ike nrụgide ga-adị elu karịa. A na-ejikarị ya agbado ihe owuwu aluminom magnesium alloy nke ụgbọ mmiri, ikpo okwu ndị dị n'ụsọ oké osimiri, locomotives na ụgbọ ala, ụgbọala, akpa, arịa cryogenic na ndị ọzọ.


Nkọwa Ngwaahịa

Akara Ngwaahịa

ER5183 dabara adaba maka ịgbado ọkụ MIG nke aluminom magnesium alloy nke na ọ dị mkpa ka ike nrụgide dị elu, ọ bụrụkwa na ígwè ntọala ya bụ 5083 ma ọ bụ 5654, ike nrụgide ahụ ga-adị elu karịa. A na-ejikarị ya agbado ọkụ nke aluminom magnesium alloy nke ụgbọ mmiri, ikpo okwu ndị dị n'ụsọ oké osimiri, locomotives na ụgbọ ala, ụgbọala, akpa, arịa cryogenic na ndị ọzọ. Ígwè ya nwere ezigbo iguzogide ire ere brine.

Ọnọdụ ịgbado ọkụ: F, HF, V

Ụdị nke Ugbu a: DCEP

ỌRỤ:

Idebe ngwugwu waya ahụ n'ọnọdụ dị mma tupu ịgbado ọkụ.

A ga-ehichapụ ma elu ala a ga-eji agwakọta ihe na waya, ihe ruru unyi nke mmanụ, ihe mkpuchi oxide, mmiri na ihe ndị ọzọ.

Iji nweta ọdịdị dị mma nke weld, ọ dị mkpa iji ọkụ ígwè isi ahụ ruo 100℃-200℃ tupu ịgbado ọkụ ma ọ bụrụ na ọkpụrụkpụ ya bụ 10mm ma ọ bụ karịa.

Ọ ka mma itinye obere efere n'okpuru mpaghara njikọta iji mee ka ígwè agbaze agbaze ahụ sie ike ka o wee hụ na ọ banye n'ime ihe njikọta ahụ kpamkpam.

Dabere na ọnọdụ ịgbado ọkụ na ọkpụrụkpụ nke ígwè isi, a ga-ahọrọ gas ọta dị iche iche, dịka 100% Ar, 75% Ar + 25% He, 50% Ar + 50% He, wdg.

Ọnọdụ ịgbado ọkụ e kwuru n'elu maka ntụaka naanị, ọ ka mma ime asambodo usoro ịgbado ọkụ dịka ọrụ ahụ si dị tupu itinye ya na ịgbado ọkụ nkịtị.

ER5183 MMIRI KEMIKỌTA nke Ígwè E tinyere (%):

SI FE CU MN MG CR ZN TI AI BE
Ọkọlọtọ ≤0.40 ≤0.40 ≤0.10 0.50-10 4.3-52 0.05-0.5 ≤0.25 ≤0.15 Nhazi nguzozi ≤0.0003
Nkịtị nkịtị 0.08 0.12 0.006 0.65 4.75 0.130 0.005 0.080 Nhazi nguzozi 0.0001

Njirimara MEKANỊKỤ nke Ígwè E tinyere (AW):

RM IKE NJIDE (MPA) MKPỤRỤ IKE REL (MPA) NKỌWA A4 (%)
Nkịtị nkịtị 280 150 18

Nha na Ọkụ A Na-atụ aro maka MIG (DC+):

Dayameta waya ịgbado ọkụ (MM) 1.2 1.6 2.0
Ọsọ ịgbado ọkụ (A) 180-300 200-400 240-450
Voltaji ịgbado ọkụ (V) 18-28 20-20 22-34

Nha na oge a na-atụ aro maka TIG (DC¯):

Dayameta waya ịgbado ọkụ (MM) 1.6-2.5 2.5-4.0 4.0-5.0
Ọsọ ịgbado ọkụ (A) 150-250 200-320 220-400

 

 

E guzobere Wenzhou Tianyu Electronic Co., Ltd. n'afọ 2000. Anyị anọwo na-emepụta elektrọd ịgbado ọkụ, mkpanaka ịgbado ọkụ, na ihe oriri ịgbado ọkụ ruo ihe karịrị afọ 20.

Ngwaahịa anyị bụ isi gụnyere elektrọd ịgbado ígwè anaghị agba nchara, elektrọd ịgbado ígwè carbon, elektrọd ịgbado ígwè dị ala, elektrọd ịgbado ọkụ n'elu, elektrọd ịgbado ígwè nickel & cobalt, waya ịgbado ígwè dị nro na nke dị ala, waya ịgbado ígwè anaghị agba nchara, waya ndị nwere ihe mkpuchi gas, waya ịgbado ígwè aluminom, waya ịgbado arc mmiri, waya ịgbado ígwè nickel & cobalt, waya ịgbado ígwè brass, waya ịgbado ígwè TIG & MIG, elektrọd tungsten, elektrọd ịgbado ígwè, na ngwa ịgbado ígwè ndị ọzọ na ihe oriri.

 

 


  • Nke gara aga:
  • Osote: