AWS ENi-C1 (Z308) Nickel dị ọcha ejiri ígwè mee ka ọ dị ọcha, Elektrọd, Mkpanaka ịgbado ọkụ, Nickel 99, Mkpanaka ịgbado ọkụ, Elektrọd Nkịtị Ni99

Nkọwa Dị Mkpirikpi:

AWS ENi-C1 (Z308) bụ elektrọd ígwè a kpụrụ akpụ nke nwere obere isi ígwè carbon yana mkpuchi graphitized siri ike.


Nkọwa Ngwaahịa

Akara Ngwaahịa

Electrode ịgbado ọkụ ígwè

Z308                                                     

GB/T EZNi-1

AWS A5.15 ENi-C1

Nkọwa: Z208 bụ elektrọd ígwè a kpụrụ akpụ nke nwere obere isi ígwè carbon yana mkpuchi graphitized siri ike. Enwere ike iji ya maka AC na DC. Njikọta ahụ nwere ike ịghọ ígwè isi awọ mgbe ọ jụrụ nwayọ nwayọ, mana ọ naghị anabata mgbawa ya nke ọma.

Ngwa: A na-eji ya arụzi ntụpọ dị na ihe e ji ígwè mee.

 

Ngwakọta kemịkalụ nke ígwè weld(%):

C

Si

Mn

S

Ni

Fe

Ndị ọzọ

≤2.0

≤2.5

≤1.0

≤0.03

≥90

≤8.0

≤1.0

 

Ugbu a akwadoro:

Dayameta mkpanaka

(mm)

2.5

3.2

4.0

Ịgbado ọkụ ugbu a

(A)

65 ~ 90

90 ~ 110

120 ~ 150

 

Rịba ama:

1. A ga-emerịrị electrode ahụ maka otu awa gburugburu 150℃ tupu ịgbado ọkụ;

2. Enwere ike iwepụ nrụgide dị n'ebe a na-arụzi ihe eji agba ọkụ site n'ịkụ ihe eji agba ọkụ iji zere mgbawa.

 

 

E guzobere Wenzhou Tianyu Electronic Co., Ltd. n'afọ 2000. Anyị anọwo na-emepụta elektrọd ịgbado ọkụ, mkpanaka ịgbado ọkụ, na ihe oriri ịgbado ọkụ ruo ihe karịrị afọ 20.

Ngwaahịa anyị bụ isi gụnyere elektrọd ịgbado ígwè anaghị agba nchara, elektrọd ịgbado ígwè carbon, elektrọd ịgbado ígwè dị ala, elektrọd ịgbado ọkụ n'elu, elektrọd ịgbado ígwè nickel & cobalt, waya ịgbado ígwè dị nro na nke dị ala, waya ịgbado ígwè anaghị agba nchara, waya ndị nwere ihe mkpuchi gas, waya ịgbado ígwè aluminom, waya ịgbado arc mmiri, waya ịgbado ígwè nickel & cobalt, waya ịgbado ígwè brass, waya ịgbado ígwè TIG & MIG, elektrọd tungsten, elektrọd ịgbado ígwè, na ngwa ịgbado ígwè ndị ọzọ na ihe oriri.

 