Nkọwa Dị Mkpirikpi:

AWS: E81T1-Ni1C-JH4, E81T1-C1A4-Ni1-H4 E mepụtara waya Flux-cored (FCAW-G) maka ngwa dị elu, nke nwere ike dị ala site na iji gas 100% CO2 protection.


Nkọwa Ngwaahịa

Akara Ngwaahịa

AWS: E81T1-Ni1C-JH4, E81T1-C1A4-Ni1-H4 Waya Flux-cored (FCAW-G)E mere ya maka ngwa dị elu, nke nwere ike dị ala site na iji gas nchekwa CO2 100%.

atụmatụ
Nwere ike imepụta ebe a na-etinye ihe ndị e ji alụ ọgụ nke nwere ike imetụta ihe karịrị 88 – 123 J (65 – 91 ft·lbf) na -40°C (-40°F)
Ezubere maka ịgbado ọkụ na gas nchekwa CO2 100%
Arụmọrụ arc kachasị elu na ọdịdị bead
Na-emezu ihe achọrọ maka iwepụ ala ọma jijiji nke AWS D1.8
nkwakọ ngwaahịa akpa foil

NKWEKỌRỊTA Nkọwapụta NKEWA
AWS AWS A5.29 E81T1-Ni1C-JH4
AWS AWS A5.36 E81T1-C1 A4-Ni1-H4
ABS ABS- Nkebi nke Abụọ 4YQ460SA H5
CWB CSA W48 E551T1-C1A4-Ni1-H4 (E551T1-Ni1C-JH4)
DNV-GL DNV-2.9 IV Y46MS H5
LR LR – Isi nke 11 4Y46S H5

NJIKỌTA EGO

Nhazi ọkwa Gas Nchedo Polarity %B %C %Cr %Mn %ọnwa %Ni %P %S %SI %V Haịdrojin A Na-agbasa
mL/100g Weld Metal
E81T1-Ni1C-JH4 100% CO2 DC+   Oke kachasị 0.12. Oke kachasị 0.15. Oke kachasị 1.5. Oke kachasị 0.35. 0.8-1.1 Oke kachasị 0.03. Oke kachasị 0.03. Oke kachasị 0.8. Oke kachasị 0.05. Oke kachasị elu nke 4.0.
E81T1-C1A4-Ni1-H4 100% CO2 DC+   Oke kachasị 0.12. Oke kachasị 0.15. Oke kachasị 1.75. Oke kachasị 0.35. 0.8-1.1 Oke kachasị 0.03. Oke kachasị 0.03. Oke kachasị 0.8. Oke kachasị 0.05. Oke kachasị 4.
Nsonaazụ nkịtị, Dịka - welded 100% CO2 DC+ 0.0050-0.006 0.04-0.05 0.04-0.06 1.12-1.42 0.01 0.81-1 Oke kachasị 0.012. Oke kachasị 0.01. 0.24-0.35 0.02- 0.03 1.7-3.2

NKỌWA
Iji mee atụmatụ ESO, wepụ 1/4 in. (6.0 mm) site na CTWD.
RỤBA AMA nke 1: Enwere ike ịchọta data nnwale mgbakwunye seismic nke ígwè FEMA na AWS D1.8 na ngwaahịa a na www.lincolnelectric.com.
RỤBA AMA nke 2: Ngwaahịa a nwere ihe ndị na-emepụta obere ihe. Enwere ike ịchọta ozi ndị ọzọ mgbe a rịọrọ ya.
E guzobere Wenzhou Tianyu Electronic Co., Ltd. na 2000. Anyị anọwo na-emepụta elektrọd ịgbado ọkụ,mkpanaka ịgbado ọkụ, na ihe eji agbado ihe karịrị afọ 20.

Ngwaahịa anyị bụ isi gụnyere elektrọd ịgbado ígwè anaghị agba nchara, elektrọd ịgbado ígwè carbon, elektrọd ịgbado ígwè dị ala, elektrọd ịgbado ọkụ n'elu, elektrọd ịgbado ígwè nickel & cobalt, waya ịgbado ígwè dị nro na nke dị ala, waya ịgbado ígwè anaghị agba nchara, waya ndị nwere ihe mkpuchi gas, waya ịgbado ígwè aluminom, waya ịgbado arc mmiri, waya ịgbado ígwè nickel & cobalt, waya ịgbado ígwè brass, waya ịgbado ígwè TIG & MIG, elektrọd tungsten, elektrọd ịgbado ígwè, na ngwa ịgbado ígwè ndị ọzọ na ihe oriri.


  • Nke gara aga:
  • Osote: