AWS E7015-G Electrode ígwè dị ala na okpomọkụ W707 mkpanaka ígwè dị ala na okpomọkụ.

Nkọwa Dị Mkpirikpi:

W707 (AWS E7015-G) bụ elektrọd ígwè dị obere okpomọkụ nwere mkpuchi sodium dị obere hydrogen.


Nkọwa Ngwaahịa

Akara Ngwaahịa

Electrọde ịgbado ígwè dị ala

W707                                                     

GB/T E5015-G

AWS A5.5 E7015-G

Nkọwa: W707 bụ elektrọd ígwè dị obere okpomọkụ nwere mkpuchi sodium dị obere hydrogen. Jiri DCEP (elektrọd direct current positive) ma nwee ike ịgbado ya n'ọnọdụ niile. Metal ahụ e tinyere ka nwere ezigbo ike mmetụta na -70°C.

Ngwa: Ejiri ya maka ịgbado ígwè dị ala dịka 2.5Ni.

 

Ngwakọta kemịkalụ nke ígwè weld(%):

C

Mn

Si

Ni

S

P

≤0.08

≤1.25

≤0.60

2.00 ~ 2.75

≤0.020

≤0.025

 

Njirimara mekaniki nke igwe weld:

Ihe nnwale

Ike ọdụdọ

Mpa

Ike mmeputa

Mpa

Ogologo

%

Uru mmetụta (J)

-70℃

Ekwere nkwa

≥490

≥390

≥22

≥27

 

Ọdịnaya hydrogen nke ígwè e tinyere n'ime ya: ≤6.0mL/100g (usoro glycerin) ma ọ bụ ≤10mL/100g (usoro mercury ma ọ bụ gas chromatography)

Nnyocha X-ray: ọkwa I

 

Ugbu a akwadoro:

(mm)

Dayameta mkpanaka

2.0

2.5

3.2

4.0

5.0

(A)

Ịgbado ọkụ ugbu a

40 ~ 70

70 ~ 100

90 ~ 120

140 ~ 180

170 ~ 210

 

Rịba ama:

1. A ga-emerịrị electrode ahụ ruo otu awa na 350℃ tupu a rụọ ọrụ ịgbado ọkụ;

2. Gbalịa iji obere ike ahịrị mgbe ị na-agbado ọkụ, ịgbado ọkụ ọtụtụ oyi akwa na ịgbado ọkụ ọtụtụ ngafe.


  • Nke gara aga:
  • Osote: