AWS E7015-G Electrode ígwè dị ala na okpomọkụ W607 Mkpanaka ịgbado ọkụ dị ala na hydrogen

Nkọwa Dị Mkpirikpi:

W607 (AWS E7015-G) bụ elektrọd ígwè dị obere okpomọkụ nwere mkpuchi sodium dị obere hydrogen


Nkọwa Ngwaahịa

Akara Ngwaahịa

Electrọde ịgbado ígwè dị ala

W607                                                     

GB/T E5015-G

AWS A5.5 E7015-G

 

Nkọwa: W607 bụ elektrọd ígwè dị obere okpomọkụ nwere mkpuchi sodium dị obere hydrogen. Jiri DCEP (elektrọd direct current positive) ma nwee ike ịgbado ya n'ọnọdụ niile. Metal ahụ e tinyere na ya nwere ezigbo ike mmetụta na -60°C.

Ngwa: Ejiri ya maka ịgbado ígwè dị ala dịka 09MnD.

 

Ngwakọta kemịkalụ nke ígwè weld(%):

C

Mn

Si

Ni

S

P

≤0.08

≤1.65

≤0.60

0.50 ~ 2.50

≤0.020

≤0.025

 

Njirimara mekaniki nke igwe weld:

Ihe nnwale

Ike ọdụdọ

Mpa

Ike mmeputa

Mpa

Ogologo

%

Uru mmetụta (J)

-60℃

Ekwere nkwa

≥490

≥390

≥22

≥27

 

Ọdịnaya hydrogen nke ígwè e tinyere n'ime ya: ≤6.0mL/100g (usoro glycerin) ma ọ bụ ≤10mL/100g (usoro mercury ma ọ bụ gas chromatography)

Nnyocha X-ray: ọkwa I

 

Ugbu a akwadoro:

(mm)

Dayameta mkpanaka

2.0

2.5

3.2

4.0

5.0

(A)

Ịgbado ọkụ ugbu a

40 ~ 70

60 ~ 90

100 ~ 120

140 ~ 170

170 ~ 200

 

Rịba ama:

1. A ga-emerịrị electrode ahụ ruo otu awa na 350℃ tupu a rụọ ọrụ ịgbado ọkụ;

2. Ọ dị mkpa ihicha ihe ndị ruru unyi, mmanụ, mmiri, na ihe ndị na-adịghị mma dị n'akụkụ ịgbado ọkụ tupu ịgbado ọkụ;

3. A pụrụ itinye akụkụ ahụ e ji agbakọta ọkụ n'ọkụ n'ihe dị ka 150°C tupu ịgbakọta ya iji gbochie mgbawa.

 


  • Nke gara aga:
  • Osote: