AWS E7015-C2L Electrode ígwè dị ala na okpomọkụ W107 Mkpanaka ịgbado ọkụ, obere hydrogen electrode ARC stick ịgbado ọkụ

Nkọwa Dị Mkpirikpi:

W107 (AWS E7015-C2L) bụ elektrọd ígwè dị obere okpomọkụ nwere mkpuchi sodium dị obere hydrogen.Jiri DCEP (electrode eletriki direct current positive) ma nwee ike ịgbado ọkụ n'ọnọdụ niile. Ígwè e tinyere n'ime ya ka nwere ezigbo ike mmetụta na -100°C.


Nkọwa Ngwaahịa

Akara Ngwaahịa

Electrọde ịgbado ígwè dị ala

W107                                                     

GB/T E5015-C2L

AWS A5.5 E7015-C2L 

Nkọwa: W107 bụ elektrọd ígwè dị ala nke nwere mkpuchi sodium dị ala nke nwere obere hydrogen.Jiri DCEP (electrode eletriki direct current positive) ma nwee ike ịgbado ọkụ n'ọnọdụ niile. Ígwè e tinyere n'ime ya ka nwere ezigbo ike mmetụta na -100°C. 

Ngwa: Ejiri ya maka ịgbado ígwè dị ala dịka 3.5Ni.

 

Ngwakọta kemịkalụ nke ígwè weld(%):

C

Mn

Si

Ni

S

P

≤0.05

≤1.25

≤0.60

3.00 ~ 3.75

≤0.020

≤0.025

 

Njirimara mekaniki nke igwe weld:

 

Ihe nnwale

 

Ike ọdụdọ

Mpa

 

Ike mmeputa

Mpa

Ogologo%

Uru mmetụta (J) -100℃

 

Ekwere nkwa

≥490

≥390

≥22

≥27

 

Ọdịnaya hydrogen nke ígwè e tinyere n'ime ya: ≤4.0mL/100g (usoro glycerin) ma ọ bụ ≤7.0mL/100g (usoro mercury ma ọ bụ gas chromatography)

 

Nnyocha X-ray: ọkwa I

 

Ugbu a akwadoro:

(mm)

Dayameta mkpanaka

2.0

2.5

3.2

4.0

5.0

(A)

Ịgbado ọkụ ugbu a

40 ~ 70

70 ~ 90

90 ~ 130

140 ~ 180

180 ~ 240

 

 

Rịba ama:

  1. A ga-emerịrị elektrọd ahụ maka otu awa na 350℃ tupu ịgbado ọkụ;
  2. Ọ dị mkpa ihicha ihe ndị ruru unyi, mmanụ, mmiri, na ihe ndị na-adịghị mma dị n'akụkụ ịgbado ọkụ tupu ịgbado ọkụ;
  3. Gbalịa iji obere ike ahịrị mgbe ị na-agbado ọkụ, ịgbado ọkụ ọtụtụ oyi akwa na ịgbado ọkụ ọtụtụ ngafe.

 