AWS E317-16 Igwe anaghị agba nchara Mkpanaka ịgbado ọkụ Arc ịgbado ọkụ Stcik Electrodes

Nkọwa Dị Mkpirikpi:

A242 (AWS E317-16) bụ elektrọd ígwè anaghị agba nchara Cr19Ni13Mo3 nke nwere obere carbon nwere mkpuchi titanium-calcium.


Nkọwa Ngwaahịa

Akara Ngwaahịa

Ịgbado ígwè anaghị agba ncharaElektrọd

A242                                      

GB/T E317-16

AWS A5.4 E317-16

Nkọwa: A242 bụ elektrọd ígwè anaghị agba nchara Cr19Ni13Mo3 dị obere nke nwere mkpuchi titanium-calcium. Enwere ike iji ya maka AC na DC ma nwee arụmọrụ dị mma. Ígwè e tinyere n'ime ya nwere ọdịnaya molybdenum dị elu karịa A202, ọ nwekwara ike iguzogide nchara ka mma megide asịd ndị na-anaghị eme ka oxidize dị ka sulfuric acid, sulfurous acid, phosphoric acid na organic acid. Ọ na-enwekwa mmetụta dị mma megide nchara na-agbawa agbawa.

Ngwa: A na-eji ya agbakọta ụdị ihe igwe anaghị agba nchara yana ígwè mejupụtara ya na ígwè dị iche iche.

 

Ngwakọta kemịkalụ nke ígwè weld(%):

C

Mn

Si

Cr

Ni

Mo

Cu

S

P

≤0.08

0.5 ~ 2.5

≤0.90

18.0 ~ 21.0

12.0 ~ 14.0

2.0 ~ 4.0

≤0.75

≤0.030

≤0.040

 

Njirimara mekaniki nke igwe weld:

Ihe nnwale

Ike ọdụdọ

Mpa

Ogologo

%

Ekwere nkwa

≥550

≥25

 

Ugbu a akwadoro:

Dayameta mkpanaka

(mm)

2.5

3.2

4.0

5.0

Ịgbado ọkụ ugbu a

(A)

50 ~ 80

80 ~ 110

110 ~ 160

160 ~ 200

 

Rịba ama:

1. A ga-emerịrị electrode ahụ ruo otu awa na 150℃ tupu a rụọ ọrụ ịgbado ọkụ;

2. Ebe ọ bụ na omimi nke ịbanye n'ime mmiri adịghị obere n'oge njikọta AC, a ga-eji ike DC mee ihe ruo n'ókè o kwere mee iji nweta ntinye miri emi. Ọkụ ekwesịghịkwa ibu oke ibu iji zere ọbara ọbara nke mkpanaka njikọta ahụ.

 

 

E guzobere Wenzhou Tianyu Electronic Co., Ltd. n'afọ 2000. Anyị anọwo na-emepụta iheelektrọd ịgbado ọkụs, mkpanaka ịgbado ọkụ, naihe eji agbado ọkụruo ihe karịrị afọ iri abụọ.

Ngwaahịa anyị bụ isi gụnyere elektrọd ịgbado ígwè anaghị agba nchara, elektrọd ịgbado ígwè carbon, elektrọd ịgbado ígwè dị ala, elektrọd ịgbado ọkụ n'elu, elektrọd ịgbado ígwè nickel & cobalt, waya ịgbado ígwè dị nro na nke dị ala, waya ịgbado ígwè anaghị agba nchara, waya ndị nwere ihe mkpuchi gas, waya ịgbado ígwè aluminom, waya ịgbado arc mmiri, waya ịgbado ígwè nickel & cobalt, waya ịgbado ígwè brass, waya ịgbado ígwè TIG & MIG, elektrọd tungsten, elektrọd ịgbado ígwè, na ngwa ịgbado ígwè ndị ọzọ na ihe oriri.

 


  • Nke gara aga:
  • Osote: