AWS A5.7 ERCuSn-C Waya Ịkwado Alloy nke ọla kọpa

Nkọwa Dị Mkpirikpi:

A na-atụ aro waya ọla kọpa Phosphor AWS A5.7 ERCuSn-C maka ịgbado ọla kọpa na ngwakọta Cu-Sn.


Nkọwa Ngwaahịa

Akara Ngwaahịa

Waya ọla nchara nke AWS A5.7 ERCuSn-C Phosphor

Okwu Mmalite
A na-atụ aro ka e jiri ọla kọpa mee ihe na-agbakọta ọla kọpa na ihe eji agbakọta ọla kọpa. Ọ kacha mma maka ịgbakọta ọla kọpa na ígwè. A na-atụ aro ka e jiri ọkụ gbaa ya tupu oge eruo maka ngwaahịa buru ibu, a na-atụkwa aro ka e jiri argon arc gbakọta ya maka iji ọtụtụ oyi akwa sie ike na ígwè.

Nhazi:   Akara ọnụọgụgụ:
GB/T9460-2008   SCu5210
AWS A5.7:2007   ERCuSn-C
BS EN14640:2005   Cu 5210
     
Nhazi (uru ọkọlọtọ):   %
Cu gụnyere.ag   bọọlụ.
Zn   0.20
Sn   7.00-9.00
Fe   0.10
P   0.10-0.35
Al   0.01
Pb   0.02
Ndị ọzọ niile   0.50
     
Njirimara anụ ahụ nke ihe:    
Njupụta Kg/m3 8.8
Oke agbaze ℃ 875-1025
Ọkwa okpomọkụ W/mK 66
Ọdụ eletriki na-eduzi Sm/mm2 6-8
Ọnụọgụ nke mgbasawanye okpomọkụ 10^-6/K(20-300℃) 18.5
     
Ụkpụrụ ọkọlọtọ nke ígwè weld:    
Ogologo % 20
Ike ọdụdọ N/mm2 260
Ọrụ mmetụta mmanya a ma ama J 32
Ike siri ike nke Brinell HB 2.5/62.5 80
     
Ngwa:    
A na-eji ígwè ọla kọpa tin nke nwere pasentị tin dị elu eme ihe, nke siri ike karịa maka ịgbado ọkụ. Ọ dabara nke ọma maka ịgbado ọkụ nke ihe ọla kọpa, dịka ọla kọpa, ọla kọpa tin, karịsịa maka ijikọ ihe ọla kọpa zinc alloys na ígwè. Ọ dị mma maka ịrụzi ịgbado ọkụ nke ọla kọpa a kpụrụ akpụ na maka ịgbado ọkụ na oven. Maka ịgbado ọkụ nke ọtụtụ oyi akwa na ígwè, a na-atụ aro ịgbado ọkụ arc pulsed. Maka nnukwu ọrụ, a na-atụ aro ka a na-ekpo ọkụ tupu oge eruo.
     
Techaa:    
Dayameta:0.64 – 0.80 – 1.00 – 1.20 – 1.60 -2.40
Spools: D100, D200, D300, D760, K300, KS300
Mkpanaka: 1.60 – 9.6 mm x 914/1000 mm
Electrodes dị.
Ị ga-eme ihe ndị ọzọ ma ọ bụrụ na ị rịọrọ ya.

E guzobere Wenzhou Tianyu Electronic Co., Ltd. n'afọ 2000. Anyị anọwo na-emepụta elektrọd ịgbado ọkụ, mkpanaka ịgbado ọkụ, na ihe oriri ịgbado ọkụ ruo ihe karịrị afọ 20.

Ngwaahịa anyị bụ isi gụnyere elektrọd ịgbado ígwè anaghị agba nchara, elektrọd ịgbado ígwè carbon, elektrọd ịgbado ígwè dị ala, elektrọd ịgbado ọkụ n'elu, elektrọd ịgbado ígwè nickel & cobalt, waya ịgbado ígwè dị nro na nke dị ala, waya ịgbado ígwè anaghị agba nchara, waya ndị nwere ihe mkpuchi gas, waya ịgbado ígwè aluminom, waya ịgbado arc mmiri, waya ịgbado ígwè nickel & cobalt, waya ịgbado ígwè brass, waya ịgbado ígwè TIG & MIG, elektrọd tungsten, elektrọd ịgbado ígwè, na ngwa ịgbado ígwè ndị ọzọ na ihe oriri.

 

 

 

 


  • Nke gara aga:
  • Osote: