Alloy Steel Welding Electrode AWS E9016-D1

Nkọwa dị mkpirikpi:

J606 (AWS E9016-D1) bụ obere alloy elu-ike ígwè electrode nwere obere-hydrogen potassium mkpuchi.Enwere ike iji ya maka ịgbado ọkụ na AC na DC niile.Nkwụsi ike arụmọrụ nke ịgbado ọkụ AC dị ala karịa nke ịgbado ọkụ DC.


Nkọwa ngwaahịa

Mkpado ngwaahịa

Ala Alloy Steel Welding Electrode

J606                                       

GB/T E6016-D1

AWS E9016-D1 

 

Description: J606 bụ obere alloy elu-ike ígwè electrode nwere obere-hydrogen potassium mkpuchi.Enwere ike iji ya maka ịgbado ọkụ na AC na DC niile.Nkwụsi ike arụmọrụ nke ịgbado ọkụ AC dị ala karịa nke ịgbado ọkụ DC. 

Ngwa: Eji maka ịgbado ọkụ ọkara carbon ígwè na ala-alloy elu-ike ígwè Ọdịdị nke kwekọrọ ekwekọ ike, dị ka Q420, wdg.

 

Ngwakọta kemịkalụ nke igwe weld (%):

C

Mn

Si

Mo

S

P

≤0.12

1.25 ~ 1.75

≤0.60

0.25 ~ 0,45

≤0.035

≤0.035

 

Njirimara nke igwe weld metal:

Nwalee ihe

Ike ọdụdọ

Mpa

Mpụta ike

Mpa

Ogologo oge

%

Uru mmetụta (J)

-30 ℃

Ekwenyere

≥590

≥490

≥15

≥27

nwalere

620 ~ 680

≥500

20 ~ 28

≥27

 

Ọdịnaya mgbasa hydrogen nke ọla edobere: ≤4.0mL/100g (usoro glycerin)

Nyocha x-ray: akara ule

 

Akwadoro ugbu a:

(mm)

Dayameta mkpanaka

2.0

2.5

3.2

4.0

5.0

5.8

(A)

Welding Ugbu a

40 ~ 70

70 ~ 90

90 ~ 120

140 ~ 180

180 ~ 220

210 ~ 260

 

Mara:

1. The electrode ga-abụọ maka 1 hour na 350 ℃ tupu ịgbado ọkụ ọrụ;

2. Ọ dị mkpa iji kpochaa nchara, ọnụ ọgụgụ mmanụ, mmiri, na adịghị ọcha na akụkụ ịgbado ọkụ tupu ịgbado ọkụ;

3. Jiri obere arc arụ ọrụ mgbe ịgbado ọkụ.Ụzọ ịgbado ọkụ dị warara kwesịrị ekwesị;

4. Mgbe akụkụ weld dị oke, a ga-ebu ụzọ kpoo ya n'elu 150 Celsius ma mee ka ọ dị jụụ nwayọọ nwayọọ mgbe ịgbado ọkụ.

 