Electrọd Ịgbado Ọkụ Na-esi Ike DIN 8555 (E1-UM-350) Mkpanaka Ịgbado Ọkụ Na-esi Ike, Electrọd Mkpanaka Na-eguzogide Iyi

Nkọwa Dị Mkpirikpi:

DIN 8555 (E1-UM-350) bụ elektrọd SMAW a kpụchara akpụcha nke ọma maka ihe na-egbochi mgbawa na iyi.


Nkọwa Ngwaahịa

Akara Ngwaahịa

Ịgbado ọkụ siri ikeElektrọd

 

Ọkọlọtọ: DIN 8555 (E1-UM-350)

Ụdị Nọmba: TY-C DUR 350

 

Nkọwapụta & Ngwa:

· Elektrọd SMAW a kpụchara akpụcha nke ọma maka ihe na-egbochi mgbawa na iyi.

· Ọ dị mma iguzogide abrasion. Ọ dị mfe ịgbado ọkụ n'ọnọdụ niile.

· Ọ dabara nke ọma maka ihe ndị na-anaghị emebi emebi n'elu akụkụ Mn-Cr-V, dịka akịrị, ihe ndị na-agbagharị egwu, ihe nkwado agbụ ígwè, wiil sprocket, ihe ndị na-eduzi egwu wdg.

 

Ngwakọta kemịkalụ nke ígwè e tinyere n'ime ya(%):

 

C

Si

Mn

Cr

Fe

DIN

-

-

-

-

-

EN

-

-

-

-

-

Nkịtị nkịtị

0.20

1.2

1.40

1.8

Bọl.

 

 

Ike nke ígwè e tinyere n'ime ya:

Dịka e siri welded

(HB)

1 oyi akwa n'elu ígwè nwere C = 0.5%

(HB)

370

420

 

Àgwà Izugbe:

· Ferrite + Martensitic nke obere usoro

· Ịrụ ọrụ dị mma na ngwaọrụ Tungsten carbide nke nwere ike itinye

· Ịkpo ọkụ tupu oge eruo Kpoo akụkụ dị arọ na ígwè ndị dị elu ruo 250-350℃

· Ịchacha Redry ruo awa abụọ na 300℃ tupu e jiri ya.

 


  • Nke gara aga:
  • Osote: