AWS/ASME 5.3 E 4047 Aluminom Welding Elektrọdes Aluminom Welding Mkpanaka Arc Welding Onye Na-ebunye Osisi Mkpanaka Arc

Nkọwa Dị Mkpirikpi:

Maka njikọta arc nke a na-ejikọta ya na ọla kọpa, silicon, na magnesium


Nkọwa Ngwaahịa

Akara Ngwaahịa

EN 573-3: E AlSi12

DIN 1732: EL-Al Si12

Atụmatụ na ngwa:

Maka njikọta arc, aluminom ejiri ọla kọpa, silicon, na magnesium gwakọta.

Ọ dịkwa mma maka ijikọ ụdị aluminom dị iche iche.

Electrọd silicon aluminum arc welding nke nwere 12% nke ihe na-ebuli onwe ya elu. E nwekwara ụdị aluminom ndị ọzọ dịka Al 99, Al Mn, wdg.

Slag pụrụ iche nke na-ebuli onwe ya elu.

Mkpuchi flux nke e si n'elu mee nke ọcha dị ọcha na-adịgide karịa ngwaahịa nkịtị n'enweghị mmiri.
Enwere ike imepụta ya n'ọtụtụ agba pụrụ iche.

A na-enweta ya na ite mgbanaka PURE ALUMINUM nke e ji hermetically mechie ma ọ bụ akpa foil e ji ihe mkpofu ekpuchi maka ogologo oge nchekwa.

A na-enwetakwa ya n'ụdị TIG dị ka koodu ihe 6047, n'ụdị MIG dị ka koodu ihe 7091 na dị ka ihe gba ọtọ.

Alloy ọkụ ọkụ dịka koodu ihe 2191:

Nyocha nke ígwè Weld niile (Ibu nkịtị%)
Agba na-agbanwe agbanwe: Ọcha ma ọ bụ Agba ahaziri ahazi
12.1 .001 .15 .01 .003 .001
Si Cu Fe Mg Mn Zn
Ịgbado ọkụ ugbu a na ntuziaka
Ugbu a akwadoro: DC Reverse (+)
Dayameta (mm) 3/32 (2.5) 1/8 (3.25)
Amperage kacha nta 50 70
Ampereji Kachasị 80 120

Usoro Ịgbado ọkụ: Malite site na iji akụkụ elu nke oke amperage. Nye elektrọd ahụ ngwa ngwa ma gaa ngwa ngwa na-ejide oghere arc dị nso.
Ọnọdụ ịgbado ọkụ: Dị larịị, Kwụ ọtọ

Ọnụego nkwụnye ego:

Dayameta (mm) Ogologo (mm) Njikọ Weld/Elektrod Electrọd kwa lb (kg) nke Weldmetal Oge Arc nke Mbelata min/lb (kg) Ntọala Amperage Ọnụego Mgbake
3/32 (2.5) 14″(350) .14oz (4.3g) 114 (251) 110 (242) 70 Pasentị iri itoolu
1/8 (3.25) 14″ (350) .23oz (6.5g) 70 (153) 62 (136) 110 Pasentị iri itoolu
5/32 (4.0) 14″ (350) .33oz (9.6g) 48 (107) 47 (103) 135 Pasentị iri itoolu

NKWEKỌTA NA NKE ELECTRODE DỊ KACHASỊ:

3/32 (2.5) 1/8 (3.25)
Ogologo (mm) 14″ (350) 14″ (350)
Electrọd / lb 49 33
Elektrọd / kg 108 73