Electrọde ịgbado ọkụ ígwè nke AWS E9016-B3 nke na-eguzogide okpomọkụ R406 Electrọde ịgbado ọkụ nke na-eguzogide oyi

Nkọwa Dị Mkpirikpi:

R406 (AWS E9016-B3) bụ elektrọd ígwè na-eguzogide okpomọkụ nke pearlitic nwere mkpuchi potassium dị obere hydrogen nke nwere 2.5% Cr – 1% Mo.


Nkọwa Ngwaahịa

Akara Ngwaahịa

Molybdenum na Chromium Molybdenum na-eguzogide okpomọkụỊkwado ígwèElektrọd

R406                                                     

GB/T E6016-B3

AWS A5.5 E9016-B3

Nkọwa: R406 bụ elektrọd ígwè nke na-eguzogide okpomọkụ pearlitic nwere mkpuchi potassium dị obere hydrogen nke nwere 2.5% Cr – 1% Mo. Enwere ike iji AC na DC mee ihe, a pụkwara ịgbado ya n'ọnọdụ niile. A ga-eme ka ịgbado ọkụ ahụ dị ọkụ ruo 160 ~ 200°C tupu ịgbado ya.

Ngwa: A na-eji ya agba ígwè Cr2.5Mo pearlitic nke na-eguzogide okpomọkụ, dịka ọkpọkọ mmiri dị elu na nke nwere okpomọkụ dị elu nke nwere okpomọkụ ọrụ dị n'okpuru 550 ° C, igwe kemịkalụ sịntetik, na ngwa mgbawa mmanụ.

 

Ngwakọta kemịkalụ nke ígwè weld(%):

C

Mn

Si

Cr

Mo

S

P

0.05 ~ 0.12

0.50 ~ 0.90

≤0.50

2.00 ~ 2.50

0.90 ~ 1.20

≤0.030

≤0.030

 

Njirimara mekaniki nke igwe weld:

Ihe nnwale

Ike ọdụdọ

Mpa

Ike mmeputa

Mpa

Ogologo

%

Uru mmetụta (J)

Ọnọdụ okpomọkụ nkịtị.

Ekwere nkwa

≥590

≥490

≥15

≥47

 

Ọdịnaya hydrogen nke ígwè e tinyere n'ime ya: ≤4.0mL/100g (usoro glycerin)

 

Nnyocha X-ray: ọkwa I

 

Ugbu a akwadoro:

Dayameta mkpanaka

(mm)

2.5

3.2

4.0

5.0

Ịgbado ọkụUgbu a

(A)

60 ~ 90

90 ~ 120

140 ~ 180

170 ~ 210

 

Rịba ama:

1. A ga-emerịrị electrode ahụ ruo otu awa na gburugburu 350℃ tupu a rụọ ọrụ ịgbado ọkụ;

2. Ọ dị mkpa ihicha ihe ndị ruru unyi, mmanụ, mmiri, na ihe ndị na-adịghị mma dị n'akụkụ ịgbado ọkụ tupu ịgbado ọkụ.

 


  • Nke gara aga:
  • Osote: