AWS E9015-B9 Mkpanaka Ịgbado Arc Mkpanaka Ịgbado Electrodes Ihe Njupụta Metal

Nkọwa Dị Mkpirikpi:

R717 (AWS E9015-B9) bụ elektrọd ígwè na-eguzogide okpomọkụ nke nwere mkpuchi sodium dị ala nke nwere 9% Cr – 1% Mo-V-Nb.


Nkọwa Ngwaahịa

Akara Ngwaahịa

Molybdenum na Chromium Molybdenum nke na-eguzogide okpomọkụ site na ígwè ịgbado ọkụ

R717                                                     

AWS A5.5 E9015-B9

Nkọwa: R717 bụ elektrọd ígwè na-eguzogide okpomọkụ nke nwere mkpuchi sodium dị ala nke nwere 9% Cr – 1% Mo-V-Nb. Jiri DCEP (elektrọd ugbu a positive) ma nwee ike ịgbado ọkụ n'ọnọdụ niile. N'ihi mgbakwunye nke obere Nb na V, ígwè e tinyere na ya nwere ezigbo iguzogide okpomọkụ dị elu.

 

Ngwa: A na-eji ya agbakọta ọkpọkọ ndị a na-ekpo oke ọkụ na isi nke ihe na-ekpo ọkụ dị elu na nke nwere nrụgide dị elu, dịka A213-T91/A335-P1 (T/P91), A387Cr, 91 na ihe owuwu ígwè ndị ọzọ na-eguzogide okpomọkụ.

Ngwakọta kemịkalụ nke ígwè weld(%):

C

Mn

Si

Cr

Mo

V

Ni

0.08 ~ 0.13

≤1.20

≤0.30

8.0 ~ 10.5

0.85 ~ 1.20

0.15 ~ 0.30

≤0.80

Nb

Cu

Al

N

S

P

 

0.02 ~ 0.10

≤0.25

≤0.04

0.02 ~ 0.07

≤0.01

≤0.01

 

Rịba ama: Mn+Ni<1.5%

 

Njirimara mekaniki nke igwe weld:

Ihe nnwale

Ike ọdụdọ

Mpa

Ike mmeputa

Mpa

Ogologo

%

Ekwere nkwa

≥620

≥530

≥17

 

Ugbu a akwadoro:

Dayameta mkpanaka

(mm)

2.5

3.2

4.0

5.0

Ịgbado ọkụ ugbu a

(A)

60 ~ 90

90 ~ 120

130 ~ 170

170 ~ 210

 

Rịba ama:

1. A ga-emerịrị electrode ahụ ruo otu awa na 350℃ tupu a rụọ ọrụ ịgbado ọkụ;

2. Ọ dị mkpa ihicha ihe ndị ruru unyi, mmanụ, mmiri, na ihe ndị na-adịghị mma dị n'akụkụ ịgbado ọkụ tupu ịgbado ọkụ.

3. Kpoo akụkụ ịgbado ọkụ ahụ ọkụ na 200 ~ 260°C tupu ịgbado ọkụ, ma debe okpomọkụ interpass kwekọrọ na ya;

4. Jiri nwayọ jụọ oyi ruo 80 ~ 100°C ruo awa abụọ mgbe ị gbanyere ya; ọ bụrụ na enweghị ike ime ọgwụgwọ okpomọkụ ozugbo enwere ike, enwere ike ịme ọgwụgwọ dehydrogenation na 350°CX awa 2.

 