AWS E8018-B2 Chromium Molybdenum Igwe Ọkụ Na-eguzogide Okpomọkụ Electrode R306Fe Stick Electrodes Ngwakọta Ịkwado Ihe Ndị A Na-eri

Nkọwa Dị Mkpirikpi:

R306Fe (AWS E8018-B2) bụ elektrọd ígwè na-eguzogide okpomọkụ nke pearlitic nwere ntụ ntụ ígwè na mkpuchi ụdị hydrogen potassium dị ala nke nwere 1% Cr - 0.5% Mo.


Nkọwa Ngwaahịa

Akara Ngwaahịa

Molybdenum na Chromium Molybdenum nke na-eguzogide okpomọkụ site na ígwè ịgbado ọkụ

R306Fe                                                     

GB/T E5518-B2

AWS A5.5 E8018-B2

Nkọwa: R306Fe bụ elektrọd ígwè na-eguzogide okpomọkụ nke pearlitic nwere ntụ ntụ ígwè na mkpuchi ụdị hydrogen potassium dị ala nke nwere 1% Cr – 0.5% Mo. Enwere ike iji ma AC na DC, a pụkwara ịgbado ya n'ọnọdụ niile site na ọrụ dị mkpirikpi. Ọkụ ọkụ nke njikọta na okpomọkụ dị n'etiti oyi akwa bụ 160 ~ 250 °C n'oge ịgbado ọkụ.

Ngwa: A na-eji ya agbakọta ígwè na-eguzogide okpomọkụ nke 1%Cr – 0.5%Mo (dịka 15CrMo), dịka ọkpọkọ elu ọkụ nke na-ekpo ọkụ nke nwere okpomọkụ ọrụ dị n'okpuru 550°C, ọkpọkọ uzuoku na arịa nrụgide nke nwere okpomọkụ ọrụ dị n'okpuru 520°C, wdg. Enwere ike iji ya agbakọta ihe nkedo ígwè nke 30CrMnSi.

 

Ngwakọta kemịkalụ nke ígwè weld(%):

C

Mn

Si

Cr

Mo

S

P

0.05 ~ 0.12

0.50 ~ 0.90

≤0.50

1.00 ~ 1.50

0.40 ~ 0.65

≤0.030

≤0.030

 

Njirimara mekaniki nke igwe weld:

Ihe nnwale

Ike ọdụdọ

Mpa

Ike mmeputa

Mpa

Ogologo

%

Uru mmetụta (J)

Ọnọdụ okpomọkụ nkịtị.

Ekwere nkwa

≥540

≥440

≥47

≥27

Anwalela

550 ~ 640

≥450

20 ~ 28

105 ~ 150

 

Ọdịnaya hydrogen nke ígwè e tinyere n'ime ya: ≤6.0mL/100g (usoro glycerin)

 

Nnyocha X-ray: ọkwa I

 

Ugbu a akwadoro:

Dayameta mkpanaka

(mm)

3.2

4.0

5.0

Ịgbado ọkụ ugbu a

(A)

100 ~ 130

140 ~ 180

180 ~ 210

 

Rịba ama:

1. A ga-emerịrị electrode ahụ ruo otu awa na gburugburu 350℃ tupu a rụọ ọrụ ịgbado ọkụ;

2. Ọ dị mkpa ihicha ihe ndị ruru unyi, mmanụ, mmiri, na ihe ndị na-adịghị mma dị n'akụkụ ịgbado ọkụ tupu ịgbado ọkụ.