AWS E8010-G Electrode Ịgbado Ọla Ala nke Alloy Steel, Onye Na-eweta Ihe Mgbado Ọla Kachasị Mma

Nkọwa Dị Mkpirikpi:

J555G (AWS E8010-G) bụ elektrọd dị elu nke nwere ihe mkpuchi sodium nke dị n'okpuru ala.


Nkọwa Ngwaahịa

Akara Ngwaahịa

Electrode ịgbado ọkụ ígwè dị ala

J555G                                               

GB/T E5510-G

AWS A5.5 E8010-G

Nkọwa: J555G bụ elektrọd dị elu nke nwere selulose sodium nke a kpuchiri n'ala. Jiri DCEP (elektrọd dị ugbu a positive). Ọ dabara maka ịgbado ọkụ kwụ ọtọ n'ala n'ọnọdụ niile nke seam okirikiri dị na ebe ọkpọkọ ahụ. Enwere ike ịgbado ya n'otu akụkụ ma mepụta ya n'akụkụ abụọ, ọsọ ịgbado ọkụ dịkwa ngwa ngwa.

Ngwa: Ejiri ya mee ihe maka ịgbado ọkụ nke ọkpọkọ ígwè dị iche iche dị ala.

 

Ngwakọta kemịkalụ nke ígwè weld(%):

C

Mn

Si

S

P

≤0.20

≥1.00

≤0.50

≤0.035

≤0.035

 

熔敷金属力学性能 Mechanical Njirimara nke weld metal:

Ihe nnwale

Ike ọdụdọ

Mpa

Ike mmeputa

Mpa

Ogologo

%

Uru mmetụta (J)

-30℃

Ekwere nkwa

≥540

≥440

≥17

≥27

Nnyocha X-ray: ọkwa nke abụọ

 

Ugbu a akwadoro:

(mm)

Dayameta mkpanaka

2.5

3.2

4.0

5.0

(A)

Ịgbado ọkụ ugbu a

40 ~ 70

70 ~ 110

110 ~ 160

160 ~ 190

 

Rịba ama:

1. Mepee ihe e ji agbakọta ihe tupu e jiri ya, ma jiri ya mee ihe dịka o kwere mee mgbe e mechara ya;

2. N'ozuzu, ọ dịghị mkpa ka a kpọọ ya ọzọ tupu a na-agbakọta ya, a pụkwara ịkpọ ya na okpomọkụ 70 ~ 90°C ruo otu awa mgbe mmiri dị.

 

E guzobere Wenzhou Tianyu Electronic Co., Ltd. n'afọ 2000. Anyị anọwo na-emepụta iheelektrọd ịgbado ọkụs, mkpanaka ịgbado ọkụ, na ihe eji agbado ihe karịrị afọ 20.

Ngwaahịa anyị bụ isi gụnyere ígwè anaghị agba ncharaelektrọd ịgbado ọkụs, elektrọd ịgbado ígwè carbon,obere elektrọd ịgbado ọkụ alloy, elektrọd ịgbado ọkụ n'elu, elektrọd ịgbado ọkụ nickel na cobalt, waya ịgbado ọkụ ígwè dị nro na nke dị ala, waya ịgbado ọkụ ígwè anaghị agba nchara, waya ndị nwere ihe mkpuchi gas, waya ịgbado ọkụ aluminom, waya ịgbado ọkụ arc dị n'ime mmiri, waya ịgbado ọkụ nickel na cobalt, waya ịgbado ọkụ brass, waya ịgbado ọkụ TIG na MIG, elektrọd tungsten, elektrọd ịgbado ọkụ carbon, na ngwa ịgbado ọkụ ndị ọzọ na ihe oriri.

 


  • Nke gara aga:
  • Osote: